Degradable polymeric compositions and articles comprising same
US-2024425683-A1 · Dec 26, 2024 · US
US2017226329A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2017226329-A1 |
| Application number | US-201515502804-A |
| Country | US |
| Kind code | A1 |
| Filing date | Aug 12, 2015 |
| Priority date | Aug 15, 2014 |
| Publication date | Aug 10, 2017 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is an aqueous composition having pH of 8 or higher and comprising (i) a solid phase comprising dispersed particles that comprise ethylcellulose polymer, (ii) fatty acid, wherein 25 mole % to 100 mole % of said fatty acid is in ionic form, (iii) 0% to 0.1% colloid stabilizer, by weight based on the dry weight of said ethylcellulose polymer, (iv) 0% to 7% plasticizer, by weight based on the dry weight of said ethylcellulose polymer, and (v) one or more cations of an alkali metal or an alkaline earth, wherein the equivalent ratio of said cations to said fatty acid is 0.1:1 to 2:1. Also provided are a method of spray drying an aqueous composition and a powder composition.
Opening claim text (preview).
1 . An aqueous composition having pH of 8 or higher and comprising (i) a solid phase comprising dispersed particles that comprise an amount of ethylcellulose polymer, (ii) 0.5% to 7% fatty acid, by weight based on the total dry weight of the solid phase, wherein 25 mole % to 100 mole % of said fatty acid is in ionic form, (iii) 0% to 0.1% colloid stabilizer, by weight based on the dry weight of said ethylcellulose polymer, (iv) 0% to 7% plasticizer, by weight based on the dry weight of said ethylcellulose polymer, and (v) one or more cations of an alkali metal or of an alkaline earth, wherein the equivalent ratio of said cations to said fatty acid is 0.1:1 to 2:1. 2 . The aqueous composition of claim 1 , wherein the amount of said ethylcellulose polymer is 45% to 90% by weight based on the dry weight of said solid phase. 3 . The aqueous composition of claim 1 , wherein said ethylcellulose powder has viscosity of 16-30 mPa-s, wherein the viscosity of said ethylcellulose powder is defined as the viscosity of a 5 weight percent solution of said ethylcellulose polymer in a solvent, based on the weight of the solution, wherein the solvent is a mixture of 80% toluene and 20% ethanol by weight based on the weight of the solvent. 4 . The aqueous composition of claim 1 , wherein the equivalent ratio of said cations to said fatty acid is 0.5:1 to 2:1. 5 . The aqueous composition of claim 1 , wherein the equivalent ratio of said cations to said fatty acid is 0.2:1 to 1:1 wherein said aqueous composition additionally comprises one or more fugitive bases, and wherein the equivalent ratio of cations of said fugitive base to said fatty acid is 0.2:1 to 1:1. 6 . A method of making a powder comprising spray drying the aqueous composition of claim 1 . 7 . A powder composition comprising (a) 0% to 2% water by weight based on the weight of said powder composition, (b) particles that comprise (I) an amount of ethylcellulose polymer, (II) 0.5% to 7% fatty acid, by weight based on the weight of said powder composition, wherein 25 mole % to 100 mole % of said fatty acid is in the form of an alkali metal or alkaline earth salt, (III) 0% to 0.1% colloid stabilizer, by weight based on the dry weight of said ethylcellulose polymer, (IV) 0% to 7% plasticizer, by weight based on the dry weight of said ethylcellulose polymer. 8 . The powder of claim 7 , wherein the amount of said ethylcellulose polymer is 45% to 90% by weight based on the dry weight of said powder. 9 . The powder composition of claim 7 , wherein said ethylcellulose powder has viscosity of 16-30 mPa-s, wherein the viscosity of said ethylcellulose powder is defined as the viscosity of a 5 weight percent solution of said ethylcellulose polymer in a solvent, based on the weight of the solution, wherein the solvent is a mixture of 80% toluene and 20% ethanol by weight based on the weight of the solvent.