Plant and method for recovering metals and/or metal oxides from industrial process waste, in particular refinery waste
US-11199360-B2 · Dec 14, 2021 · US
US2017204495A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2017204495-A1 |
| Application number | US-201515328619-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jul 10, 2015 |
| Priority date | Aug 1, 2014 |
| Publication date | Jul 20, 2017 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for smelting nickel oxide ore according to the present invention uses pellets of nickel oxide ore and is characterized by comprising: a pellet production step S 1 for producing pellets from nickel oxide ore; a reduction step S 2 for heating the resulting pellets at a predetermined reduction temperature in a reduction furnace to obtain a mixture of iron-nickel alloy and slag; and a separation step S 3 for separating out and recovering the iron-nickel alloy form the resulting mixture, the separation step S 3 comprising the creation of pulverized matter by pulverizing the mixture so that at least the slag becomes smaller than 2 mm, and sorting the resulting pulverized matter with a magnetic force of 300 to 600 gauss.
Opening claim text (preview).
1 . A method for smelting nickel oxide ore using pellets of nickel oxide ore, the method comprising: a pellet production step of producing pellets from the nickel oxide ore; a reduction step of obtaining a mixture of iron-nickel alloy and slag, by heating the pellets obtained at a predetermined reduction temperature with a reducing furnace; and a separation step of separating and recovering the iron-nickel alloy from the mixture obtained, wherein the mixture is pulverized so that at least the slag becomes a size less than 2 mm to make a pulverized material, and the pulverized material thus obtained is sorted with a magnetic force of 300 Gauss to 600 Gauss in the separation step. 2 . The method for smelting nickel oxide ore according to claim 1 , wherein the nickel oxide ore is limonite or saprolite. 3 . A method for separating and recovering an iron-nickel alloy by separating and recovering the iron-nickel alloy from a mixture of the iron-nickel alloy and slag obtained by subjecting pellets of nickel oxide ore to a reducing heat treatment, the method comprising: pulverizing the mixture so that at least the slag becomes a size less than 2 mm; and sorting a pulverized material obtained by pulverizing with a magnetic force of 300 Gauss to 600 Gauss.
by reduction in solid state, e.g. by segregation processes · CPC title
enduration of pellets · CPC title
with formation of ferro-nickel or ferro-cobalt · CPC title
with carbonaceous material for the production of coked agglomerates · CPC title