Method and device for hot stamping
US-9511619-B2 · Dec 6, 2016 · US
US2017129271A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2017129271-A1 |
| Application number | US-201715412218-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jan 23, 2017 |
| Priority date | Dec 7, 2007 |
| Publication date | May 11, 2017 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention relates to a method for producing a security and/or valuable document containing a polymer layer composite or consisting thereof, said polymer layer composite being formed from a polymer layer partial composite and a polymer cover layer and the polymer layer partial composite and/or the polymer cover layer containing a laser sensitive component, consisting of the followings steps: A) first personalized information is applied to the polymer layer partial composite by means of an inkjet printing method as a colored inkjet printed layer, B) the polymer cover layer is applied to the inkjet printed layer and is joined to the polymer layer partial composite by thermal lamination, and C) second personalized information is inscribed into the polymer layer composite of the security and/or valuable document, obtained in step B), by means of laser engraving. The invention also relates to a security and/or valuable document that can be produced according to said method.
Opening claim text (preview).
1 . A method for producing a security and/or valuable document containing a polymer layer composite or consisting thereof, said polymer layer composite being formed from a polymer layer partial composite comprising a first polymer and a polymer cover layer comprising a second polymer, the polymer layer partial composite and/or the polymer cover layer containing a laser sensitive component, wherein the method comprises A) applying first personalized information to the polymer layer partial composite by means of an inkjet printing method as a colored inkjet printed layer, B) applying the polymer cover layer to the inkjet printed layer with subsequent joining to the polymer layer partial composite by thermal lamination, and either C1) inscribing second personalized information into the polymer layer composite of the security and/or valuable document obtained in step B) by means of laser engraving, or C2) inscribing second personalized information into the polymer layer partial composite, before one of steps A) or B), by means of laser engraving. 2 . The method according to claim 1 , wherein the polymer cover layer is formed from a polymer with a glass temperature before the lamination of less than 140° C. 3 . The method according to claim 1 , wherein (a) the polymer layer partial composite and the polymer cover layer are formed from identical or different polymers, (b) the polymer cover layer and optionally the polymer layer partial composite each contain identical or different groups that are reactive with each other, and (c) the reactive groups of the polymer cover layer are reacted with each other and/or the reactive groups of the polymer layer partial composite at a lamination temperature of less than 200° C. and undergo covalent binding with each other. 4 . The method according to claim 2 , wherein the glass temperature of the polymer cover layer before the thermal lamination is less than 120° C., and wherein the glass temperature of the polymer cover layer after the thermal lamination by reaction of reactive groups of the basic polymer of the polymer cover layer with each other is at least by 5° C., higher than the glass temperature before the thermal lamination. 5 . The method according to claim 3 , wherein the lamination temperature in step B) is less than 180° C. 6 . The method according to claim 1 , wherein the polymers of the polymer partial composite and of the polymer cover layer are identical or different and are formed from a polymer selected from the group consisting of polycarbonate, polyethylene glycol terephthalate, polymethyl methacrylate, thermoplastic polyurethane elastomers, polyethylene, polypropylene, polyimide or poly-trans-isoprene, and copolymers of the foregoing polymers. 7 . The method according to claim 6 , wherein the polymer partial composite and/or the polymer cover layer are formed from the polycarbonate. 8 . The method according to claim 3 , wherein the reactive groups for each polymer are selected from the group consisting of —CN, —OCN, —NCO, —NC, —SH, —S x , -Tos, —SCN, —NCS, —H, epoxy (—CHOCH 2 ), —NH 2 , —NN+, —NN—R, —OH, —COOH, —CHO, —COOR, -Hal, -Me-Hal, —Si(OR) 3 , —SiHal 3 , —CH═CH 2 , and —COR, wherein R may be a reactive or non-reactive group selected from —H, -Hal, C 1 -C 20 alkyl, C 3 -C 20 aryl, C 4 -C 20 aralkyl, each branched or linear, saturated or unsaturated, optionally substituted, or corresponding heterocycles with one or several, identical or different heteroatoms selected from O, N and S. 9 . The method according to claim 3 , wherein the reactive groups are connected by a spacer group to the polymer, said spacer group being selected from the group consisting of —(CH 2 )n-, —(CH 2 —CH 2 —O) n —, —(SiR 2 —O) n —, —(C 6 H 10 ) n —, —(C 6 H 10 ) n —, C 1 -C n alkyl, C 3 -C (n+3) aryl, C 4 -C (n+4) aralkyl, each branched or linear, saturated or unsaturated, optionally substituted, or corresponding heterocycles with one or several, identical or different heteroatoms selected from O, N and S with n=1 to 20. 10 . The method according to claim 1 , wherein the polymer layer partial composite contains an electronic circuit, and wherein a third personalized information is stored before, at the same time or after step C) in the electronic circuitry. 11 . The method according to claim 1 , wherein the polymer cover layer comprises a laser sensitive component. 12 . The method according to claim 1 , wherein the first personalized information is a color portion of a personalized overall picture information, and wherein the second personalized information is a black portion of the personalized overall picture information. 13 . The method according to claim 1 , wherein an optical inspection of the colored inkjet printed layer and/or an electronic test of the electronic circuit is made before or after step B) or C). 14 .- 23 . (canceled)
using heat · CPC title
Ablative recording, e.g. by burning marks; Spark recording {(marking by high energetic means, e.g. by laser otherwise than burning or ablative removal B41M5/26; materials or methods for recording or reproduction by optical means G11B7/00)} · CPC title
Security printing {(securities B42D25/29)} · CPC title
Layered products comprising {a layer of} synthetic resin {(fibrous or filamentary layer made of a synthetic resin B32B5/02; particulate layer made of a synthetic resin B32B5/16; foamed layer made of a synthetic resin B32B5/18)} · CPC title
by ink-jet printing · CPC title