Photovoltaic module backsheet comprising polyolefin layers
US-2024063320-A1 · Feb 22, 2024 · US
US2016347940A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016347940-A1 |
| Application number | US-201514957519-A |
| Country | US |
| Kind code | A1 |
| Filing date | Dec 2, 2015 |
| Priority date | May 29, 2015 |
| Publication date | Dec 1, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A polypropylene resin composition having high transparency and heat-resistance comprises: 100 parts by weight of a matrix resin composition comprising 60 to 70 wt % homo-polypropylene and 30 to 40 wt % random-polypropylene; 0.3 to 0.5 parts by weight of an antioxidant; 0.3 to 0.5 parts by weight of a heat-resistance stabilizer; 0.2 to 0.5 parts by weight of a lubricant; and 0.2 to 0.5 parts by weight of a nucleating agent.
Opening claim text (preview).
What is claimed is: 1 . A polypropylene resin composition having high transparency and heat-resistance comprising: 100 parts by weight of a matrix resin composition comprising 60 to 70 wt % homo-polypropylene and 30 to 40 wt % random-polypropylene; 0.3 to 0.5 parts by weight of an antioxidant; 0.3 to 0.5 parts by weight of a heat-resistance stabilizer; 0.2 to 0.5 parts by weight of a lubricant; and 0.2 to 0.5 parts by weight of a nucleating agent. 2 . The polypropylene resin composition of claim 1 , wherein the homo-polypropylene has a melt index of 1 to 10 g/10 min and a softening point of 130 to 180° C. 3 . The polypropylene resin composition of claim 1 , wherein the random-polypropylene has a melt index of 10 to 20 g/10 min and a softening point of 100 to 160° C. 4 . The polypropylene resin composition of claim 1 , wherein the antioxidant is a phenol-based compound, a phosphorus compound, or a mixture thereof. 5 . The polypropylene resin composition of claim 1 , wherein the heat-resistance stabilizer is at least one selected from the group consisting of a sulfur-based compound, a phenol-based compound, and a phosphorous-based compound. 6 . The polypropylene resin composition of claim 1 , wherein the lubricant is an olefin-based compound. 7 . The polypropylene resin composition of claim 1 , wherein the nucleating agent is at least one selected from the group consisting of benzylidene sorbitol, methylbenzylidene sorbitol, ethylbenzylidene sorbitol, and di(p-methylbenzylidene) sorbitol.
Polypropene · CPC title
Transparent films; Clear coatings; Transparent materials · CPC title
Copolymers of propene (C08L23/16 takes precedence) · CPC title
Sulfides {, e.g. R-(S)x-R'} · CPC title
Carboxylic acid amides · CPC title
Related publications grouped by family.