Low firing temperature dielectric materials designed to be co-fired with high bismuth garnet ferrites for miniaturized isolators and circulators
US-2019393579-A1 · Dec 26, 2019 · US
US2016300651A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016300651-A1 |
| Application number | US-201615090196-A |
| Country | US |
| Kind code | A1 |
| Filing date | Apr 4, 2016 |
| Priority date | Apr 2, 2015 |
| Publication date | Oct 13, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A ferrite composition composed of a main component including 26 to 46 mol % of an iron oxide in terms of Fe 2 O 3 , 4 to 14 mol % of a copper oxide in terms of CuO, 0 to 26 mol % of a zinc oxide in terms of ZnO, and a residue of 40.0 mol % or more of a nickel oxide in terms of NiO. The ferrite composition, with respect to 100 parts by weight of the main component, is also composed of a subcomponent including 0.8 to 10.0 parts by weight of a silicon compound in terms of SiO 2 , 1.0 to 15.0 parts by weight of a cobalt compound in terms of Co 3 O 4 , and 0.7 to 30.0 parts by weight of a bismuth compound in terms of Bi 2 O 3 . A value of the cobalt compound content in terms of Co 3 O 4 divided by the silicon compound content in terms of SiO 2 is 0.4 to 5.5.
Opening claim text (preview).
1 . A ferrite composition comprising a main component and a subcomponent, in which the main component comprises 26 to 46 mol % of an iron oxide in terms of Fe 2 O 3 , 4 to 14 mol % of a copper oxide in terms of CuO, 0 to 26 mol % of a zinc oxide in terms of ZnO, and a residue of 40.0 mol % or more of a nickel oxide in terms of NiO, the subcomponent comprises 0.8 to 10.0 parts by weight of a silicon compound in terms of SiO 2 , 1.0 to 15.0 parts by weight of a cobalt compound in terms of Co 3 O 4 , and 0.7 to 30.0 parts by weight of a bismuth compound in terms of Bi 2 O 3 , with respect to 100 parts by weight of the main component, and a ratio of a content of the cobalt compound in terms of Co 3 O 4 divided by a content of the silicon compound in terms of SiO 2 is 0.4 to 5.5. 2 . An electronic component comprising a ferrite sintered body composed of the ferrite composition as set forth in claim 1 .
on stacked layers · CPC title
Printed windings · CPC title
[(TO4) 3] with T= Si, Al, Fe, Ga (H01F10/24 takes precedence; Faraday rotators G02F1/09) · CPC title
Thermal treatment of powders or mixtures thereof other than sintering · CPC title
Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.