Method for preparing titanium nitride-titanium diboride-cubic boron nitride composite material

US2016297713A1 · US · A1

Patent metadata
FieldValue
Publication numberUS-2016297713-A1
Application numberUS-201415100857-A
CountryUS
Kind codeA1
Filing dateJun 27, 2014
Priority dateJun 9, 2014
Publication dateOct 13, 2016
Grant date

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A method for preparing a titanium nitride-titanium diboride-cubic boron nitride composite material is disclosed. Titanium powder and cubic boron nitride raw powders are mixed by a planetary ball milling method, and then the titanium nitride-titanium diboride-cubic boron nitride composite material is prepared through the steps of wet mixing, drying, sieving, pre-sintering through a high-temperature vacuum furnace, cold isostatic press molding and high-temperature sintering.

First claim

Opening claim text (preview).

1 . A method for preparing a titanium nitride-titanium diboride-cubic boron nitride composite material, comprising: (1) adopting Ti powder and cBN powder as raw materials, and utilizing in-situ reaction to prepare the titanium nitride-titanium diboride-cubic boron nitride composite material, wherein the reaction equation is as follows: ( 1 - x )  Ti + 2 + x 3  c  BN → 2  ( 1 - x ) 3  Ti  N + ( 1 - x ) 3  Ti  B 2 + x  cBN , ( I ) wherein x is the mole content of cBN, and the weights of the Ti powder and cBN powder are calculated according to the following formulas: V TiN = ( 1 - V cBN ) × ( 2 × M TiN ρ TiN 2 × M TiN ρ TiN + M TiB   2 ρ TiB   2 ) , ( II ) ; V TiB   2 = ( 1 - V cBN ) × ( M TiB 

Assignees

Inventors

Classifications

  • based on cubic boron nitrides {or Wurtzitic boron nitrides, including crystal structure transformation of powder} · CPC title

  • Refractory metals · CPC title

  • based on titanium nitrides, e.g. TiAlON · CPC title

  • Heating rate · CPC title

  • micrometer sized, i.e. from 1 to 100 micron · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US2016297713A1 cover?
A method for preparing a titanium nitride-titanium diboride-cubic boron nitride composite material is disclosed. Titanium powder and cubic boron nitride raw powders are mixed by a planetary ball milling method, and then the titanium nitride-titanium diboride-cubic boron nitride composite material is prepared through the steps of wet mixing, drying, sieving, pre-sintering through a high-temperat…
Who is the assignee on this patent?
Univ Hohai
What technology area does this patent fall under?
Primary CPC classification C04B35/5831. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Thu Oct 13 2016 00:00:00 GMT+0000 (Coordinated Universal Time) (A1). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).