Polarizer and polarizing plate including same
US-2017003426-A1 · Jan 5, 2017 · US
US2016238770A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016238770-A1 |
| Application number | US-201615042599-A |
| Country | US |
| Kind code | A1 |
| Filing date | Feb 12, 2016 |
| Priority date | Feb 16, 2015 |
| Publication date | Aug 18, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A polarizer according to an embodiment of the present invention includes a resin film having a thickness of 13 μm or less and containing iodine. The resin film has formed therein a low-concentration portion having a content of the iodine lower than that of another portion.
Opening claim text (preview).
What is claimed is: 1 . A polarizer, comprising a resin film having a thickness of 13 μm or less and containing iodine, wherein the resin film has formed therein a low-concentration portion having a content of the iodine lower than that of another portion. 2 . The polarizer according to claim 1 , wherein the polarizer has a single axis transmittance of 42.0% or more and a polarization degree of 99.95% or more in the another portion. 3 . The polarizer according to claim 1 , wherein the low-concentration portion has a transmittance of 50% or more. 4 . The polarizer according to claim 1 , wherein the content of the iodine in the low-concentration portion is 1.0 wt % or less. 5 . The polarizer according to claim 1 , wherein the low-concentration portion has a substantially circular shape having a diameter of 10 mm or less. 6 . The polarizer according to claim 1 , wherein the thickness of the resin film is 8 μm or less. 7 . The polarizer according to claim 1 , wherein the low-concentration portion corresponds to a camera hole portion of an image display apparatus on which the polarizer is mounted. 8 . The polarizer according to claim 1 , wherein the low-concentration portion is formed by bringing a basic solution into contact with the resin film containing the iodine. 9 . The polarizer according to claim 8 , wherein the basic solution comprises an aqueous solution of sodium hydroxide having a concentration of 1 wt. % or more. 10 . A polarizing plate, comprising the polarizer of claim 1 . 11 . An image display apparatus, comprising the polarizing plate of claim 10 . 12 . A method of producing the polarizer of claim 1 , the method comprising bringing a basic solution into contact with a resin film having a thickness of 13 μm or less and containing iodine. 13 . The production method according to claim 12 , wherein the basic solution has a temperature of 20° C. or more. 14 . The production method according to claim 12 , further comprising bringing an acidic solution into contact with a portion of the resin film with which the basic solution has been brought into contact. 15 . The production method according to claim 12 , wherein the resin film comprises a resin layer formed on a substrate. 16 . The production method according to claim 15 , wherein the resin layer comprises an applied layer.
in the form of a thin sheet or foil, e.g. Polaroid · CPC title
including organic materials, e.g. polymeric layers · CPC title
Filters employing polarising elements, e.g. Lyot or Solc filters (G02B5/3016 takes precedence) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.