Can manufacturing method, can manufacturing device, can, and can manufacturing tool set
US-2021308736-A1 · Oct 7, 2021 · US
US2016236261A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016236261-A1 |
| Application number | US-201415026049-A |
| Country | US |
| Kind code | A1 |
| Filing date | Sep 30, 2014 |
| Priority date | Sep 30, 2013 |
| Publication date | Aug 18, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A system and method of forming a metal container with a featured sidewall may include providing a blow molded metal container. The metal container may be positioned into a mold inclusive of at least one sidewall feature. The metal container may be blow molded again to cause the at least one sidewall feature to be created in the sidewall of the container as defined by the mold. In one embodiment, a sidewall of the metal container may be at least partially annealed. The sidewall feature may include a portion of a profile of a sporting good, such as a baseball, embossed feature (e.g., word), logo, or otherwise. The metal container may be a shaped metal container.
Opening claim text (preview).
1 . A method of forming a container with a featured sidewall, said method comprising: providing a blow molded metal container; positioning the metal container into a mold inclusive of at least one sidewall feature; and blow molding the metal container again to cause the at least one sidewall feature to be created in a sidewall of the metal container as defined by the mold. 2 . The method according to claim 1 , wherein providing the metal container includes providing a partially formed metal container. 3 . The method according to claim 1 , wherein providing the metal container includes providing a fully formed metal container. 4 . The method according to claim 1 , further comprising at least partially annealing the sidewall of the metal container. 5 . The method according to claim 4 , wherein at least partially annealing includes heating the sidewall to a temperature that causes metal grains of the sidewall transition to a reduced stress state from an existing stress state. 6 . The method according to claim 5 , wherein at least partially annealing the sidewall includes at least partially annealing a localized portion of the sidewall. 7 . The method according to claim 1 , wherein positioning the metal container in the mold includes moving a plurality of mold pieces about the metal container, the mold pieces, when integrated or in contact with one another, having a profile that substantially matches a profile of the metal container with the exception of the at least one sidewall feature of the mold. 8 . The method according to claim 1 , wherein the at least one sidewall feature includes a portion of a profile of a sporting good. 9 . The method according to claim 1 , wherein the at least one sidewall feature includes an embossed feature. 10 . The method according to claim 9 , wherein the embossed feature includes a word. 11 . The method according to claim 1 , wherein the metal at the at least one sidewall feature has a different hardness than metal surrounding the at least one sidewall feature. 12 . The method according to claim 1 , wherein providing the blow molded metal container includes providing a shaped metal container in a shape of a bottle. 13 . A system for forming a metal container with a featured sidewall, said system comprising: providing a mold inclusive of at least one sidewall feature, and adapted to receive a blow molded metal container; and a blowing mechanism configured to blow mold the metal container again to cause the at least one sidewall feature to be created in a sidewall of the metal container as defined by the mold. 14 . The system according to claim 13 , wherein the metal container is a partially formed metal container. 15 . The system according to claim 13 , wherein the metal container is a fully formed metal container. 16 . The system according to claim 13 , further comprising a heater configured to at least partially anneal the sidewall of the metal container. 17 . The system according to claim 16 , wherein the heater is configured to at least partially anneal the sidewall to a temperature that causes metal grains of the sidewall to transition to a reduced stress state from an existing stress state. 18 . The system according to claim 16 , wherein the at least partially annealed sidewall is heated in a localized portion of the sidewall. 19 . The system according to claim 13 , wherein the mold includes a plurality of mold pieces configured to be formed about the metal container, the mold pieces, when integrated or in contact with one another, having a profile that substantially matches a profile of the metal container with the exception of the at least one sidewall feature of the mold. 20 . The system according to claim 13 , wherein the at least one sidewall feature includes a portion of a profile of a sporting good. 21 - 24 . (canceled)
Deforming bodies having a closed end · CPC title
Locally embossing the walls of formed can bodies (B44B5/00, B44C1/24, B44C3/085 take precedence; bulging B21D51/2646) · CPC title