Method for producing chemically strengthened glass

US2016207828A1 · US · A1

Patent metadata
FieldValue
Publication numberUS-2016207828-A1
Application numberUS-201615000675-A
CountryUS
Kind codeA1
Filing dateJan 19, 2016
Priority dateJul 19, 2013
Publication dateJul 21, 2016
Grant date

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A method for producing a chemically strengthened glass, including a step of bringing a glass containing sodium into contact with an inorganic salt containing potassium nitrate, thereby performing ion exchange of a Na ion in the glass with a K ion in the inorganic salt, in which the inorganic salt contains at least one salt selected from the group consisting of K 2 CO 3 , Na 2 CO 3 , KHCO 3 , NaHCO 3 , K 3 PO 4 , Na 3 PO 4 , K 2 SO 4 , Na 2 SO 4 , KOH and NaOH, and the method includes: a step of washing the glass after the ion exchange; a step of subjecting the glass to an acid treatment after the washing; and a step of subjecting the glass to an alkali treatment after the acid treatment.

First claim

Opening claim text (preview).

1 . A method for producing a chemically strengthened glass, comprising a step of bringing a glass containing sodium into contact with an inorganic salt containing potassium nitrate, thereby performing ion exchange of a Na ion in the glass with a K ion in the inorganic salt, wherein the inorganic salt contains at least one salt selected from the group consisting of K 2 CO 3 , Na 2 CO 3 , KHCO 3 , NaHCO 3 , K 3 PO 4 , Na 3 PO 4 , K 2 SO 4 , Na 2 SO 4 , KOH and NaOH, and the method comprises:…

Assignees

Inventors

Classifications

  • Chemistry & Metallurgy · mapped topic

  • Chemistry & Metallurgy · mapped topic

  • Chemistry & Metallurgy · mapped topic

  • Chemistry & Metallurgy · mapped topic

  • Chemistry & Metallurgy · mapped topic

Patent family

Related publications grouped by family.

External sources

Next steps

Free tools are coming soon. Tell us what you want to track and we'll notify you.

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US2016207828A1 cover?
A method for producing a chemically strengthened glass, including a step of bringing a glass containing sodium into contact with an inorganic salt containing potassium nitrate, thereby performing ion exchange of a Na ion in the glass with a K ion in the inorganic salt, in which the inorganic salt contains at least one salt selected from the group consisting of K 2 CO 3 , Na 2 CO 3 , KHCO 3 , Na…
Who is the assignee on this patent?
Asahi Glass Co Ltd
What technology area does this patent fall under?
Primary CPC classification C03C21/002. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Thu Jul 21 2016 00:00:00 GMT+0000 (Coordinated Universal Time) (A1). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).