Composite metal oxide, method for producing composite metal oxide, and sodium secondary battery
US-2015333363-A1 · Nov 19, 2015 · US
US2016190551A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016190551-A1 |
| Application number | US-201414903483-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jun 18, 2014 |
| Priority date | Jul 10, 2013 |
| Publication date | Jun 30, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a mixed active material for a lithium secondary battery, which includes a lithium transition metal composite oxide having an α-NaFeO 2 structure with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5, and a lithium transition metal composite oxide having an α-NaFeO 2 structure with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0 and not more than 0.5, wherein the mixed active material has a specific surface area of 4.4 m 2 /g or less and a S content of 0.2 to 1.2% by mass.
Opening claim text (preview).
1 . A mixed active material for a lithium secondary battery, which comprises: a lithium transition metal composite oxide having an α-NaFeO 2 structure with a transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5, and a lithium transition metal composite oxide having an α-NaFeO 2 structure with a transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0 and not more than 0.5, wherein the mixed active material has a specific surface area of 4.4 m 2 /g or less and a S content of 0.2 to 1.2% by mass. 2 . The mixed active material for a lithium secondary battery according to claim 1 , wherein S is incorporated by acid-treating the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0 and not more than 0.5. 3 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the mixing ratio of the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 and the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0 and not more than 0.5 is 70:30 to 95:5. 4 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the mixing ratio of the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 and the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0 and not more than 0.5 is 80:20 to 90:10. 5 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Co/Me molar ratio (molar ratio of Co to the transition metal Me) of 0.05 to 0.40. 6 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Co/Me molar ratio (molar ratio of Co to the transition metal Me) of 0.10 to 0.30. 7 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the specific surface area is 4.2 m 2 /g or less. 8 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the specific surface area is 3.8 m 2 /g or less. 9 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the S content is 0.2 to 1.0% by mass. 10 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the S content is 0.2 to 0.8% by mass. 11 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has the Mn/Me molar ratio of more than 0.5 and not more than 0.8. 12 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has the Mn/Me molar ratio of more than 0.5 and not more than 0.75. 13 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Li/Me molar ratio (molar ratio of lithium (Li) to the transition metal) of more than 1. 14 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Li/Me molar ratio (molar ratio of lithium (Li) to the transition metal) of more than 1.2. 15 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Li/Me molar ratio (molar ratio of lithium (Li) to the transition metal) of more than 1.2 and less than 1.6. 16 . The mixed active material for a lithium secondary battery according to claim 1 , wherein the lithium transition metal composite oxide with the transition metal (Me) including Co, Ni and Mn and the Mn/Me molar ratio being more than 0.5 has a Li/Me molar ratio (molar ratio of lithium (Li) to the transition metal) of not less than 1.25 and not more than 1.5. 17 . A lithium secondary battery electrode comprising the mixed active material for a lithium secondary battery according to claim 1 . 18 . A lithium secondary battery comprising the lithium secondary battery electrode according to claim 17 . 19 . A power storage apparatus in which the plurality of lithium secondary batteries according to claim 18 are assembled to construct the power storage apparatus.
Pore diameter · CPC title
Li-accumulators · CPC title
Pore volume · CPC title
as mixtures · CPC title
by peak-intensities or a ratio thereof only · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.