Mixture, use of this mixture, and method for conditioning a slag located on a metal melt in a metallurgical vessel in iron and steel metallurgy
US-2017275714-A1 · Sep 28, 2017 · US
US2016130674A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016130674-A1 |
| Application number | US-201514967520-A |
| Country | US |
| Kind code | A1 |
| Filing date | Dec 14, 2015 |
| Priority date | Dec 28, 2006 |
| Publication date | May 12, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A Si-killed steel wire rod for obtaining a spring excellent in fatigue properties and a spring excellent in fatigue properties obtained from such steel wire rod are provided. In the Si-killed steel wire rod of the present invention, oxide-based inclusions present in the wire rod contain SiO 2 : 30-90%, Al 2 O 3 : 2-35%, MgO: 35% or below (not inclusive of 0%), CaO: 50% or below (not inclusive of 0%), MnO: 20% or below (not inclusive of 0%) and BaO: 0.2-20% respectively, and total content of (CaO+MgO) is 3% or above.
Opening claim text (preview).
1 . A Si-killed steel wire rod excellent in fatigue properties, wherein oxide-based inclusions present in the wire rod comprise in mass % SiO 2 : 30-90%, Al 2 O 3 : 2-35%, MgO: 35% or below (not inclusive of 0%), CaO: 50% or below (not inclusive of 0%), MnO: 20% or below (not inclusive of 0%) and BaO: 0.2-20% respectively, and the total content of (MgO+CaO) is 3% or above. 2 . The Si-killed steel wire rod as set forth in claim 1 , wherein oxide-based inclusions present in the wire rod further comprise Li 2 O in a range of 0.1-20%. 3 . The Si-killed steel wire rod as set forth in claim 1 , composed of steel comprising C: 1.2% or below (not inclusive of 0%), Si: 0.1-4.0%, Mn: 0.1-2.0%, and Al: 0.01% or below (not inclusive of 0%) respectively. 4 . The Si-killed steel wire rod as set forth in claim 3 , further comprising one or more elements selected from a group consisting of Cr, Ni, V, Nb, Mo, W, Cu, Ti, Co and a rare earth element. 5 . The Si-killed steel wire rod as set forth in claim 3 , wherein the balance is Fe and inevitable impurities. 6 . A spring obtained from the Si-killed steel wire rod as set forth in claim 1 .