R-T-B based sintered magnet
US-9520216-B2 · Dec 13, 2016 · US
US2016104573A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016104573-A1 |
| Application number | US-201514974707-A |
| Country | US |
| Kind code | A1 |
| Filing date | Dec 18, 2015 |
| Priority date | Jun 18, 2013 |
| Publication date | Apr 14, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a method for manufacturing an Nd—Fe—B-based permanent magnet having an improved coercive force while reducing the amount of Dy used. A method for manufacturing a permanent magnet according to an embodiment of the present invention may comprise the steps of: preparing powder including Nd, Fe, B, and Cu; preparing a shaped body by forming a specific magnetic field in the powder; sintering the shaped body at a specific sintering temperature; and subjecting the sintered, shaped body to annealing at a annealing temperature determined according to the content of Cu.
Opening claim text (preview).
What is claimed is: 1 . A method for manufacturing a permanent magnet, which comprises: preparing powder including Nd, Fe, B and Cu; preparing a shaped body by forming a specific magnetic field in the powder; sintering the shaped body at a specific sintering temperature; and subjecting the sintered, shaped body to annealing at an annealing temperature determined according to the Cu content. 2 . The method for manufacturing a permanent magnet of claim 1 , wherein the annealing step comprises a plurality of annealings, and the annealing temperature determined according to the content of Cu is a first annealing of the plurality of annealings. 3 . The method for manufacturing a permanent magnet of claim 1 , wherein the content of Cu is 0.01 to 0.8 weight ratio to the powder. 4 . The method for manufacturing a permanent magnet of claim 3 , wherein the annealing temperature determined by the content of Cu is reduced as the content of Cu is increasing. 5 . The method for manufacturing a permanent magnet of claim 1 , wherein the specific sintering temperature is determined according to the content of Cu.
Treatment of metallic powder (mixing with lubricating or binding agents or with organic material B22F1/10) · CPC title
Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties · CPC title
Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00 · CPC title
Aluminium · CPC title
containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60 · CPC title