Solid-state lithium-ion conductor and methods of manufacture thereof
US-11876225-B2 · Jan 16, 2024 · US
US2015132658A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2015132658-A1 |
| Application number | US-201314402501-A |
| Country | US |
| Kind code | A1 |
| Filing date | May 21, 2013 |
| Priority date | May 22, 2012 |
| Publication date | May 14, 2015 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
An object of the present invention is to provide a copper foil inexpensive and sufficient in tensile strength even after heat treatment. The copper foil includes zinc in a content range of 0.02% by mass to 2.7% by mass in the total mass of the entire copper foil, and if the regions in thicknesses direction from both surfaces of the copper foil where occupies 5% by mass in the total mass of the entire copper foil are referred to as the respective external layers and a region between one external layer and the other external layer is referred to as an internal layer, the internal layer includes copper as a main element and includes 100 ppm or more of one or mixture of small amount-elements selected from carbon, sulfur, chlorine and nitrogen, and includes zinc at 10% or more in the total mass of zinc included in the entire copper foil.
Opening claim text (preview).
1 . A copper foil including zinc in a content range of 0.02% by mass to 2.7% by mass in the total mass of the entire copper foil, wherein the regions in thicknesses direction from both surfaces of the copper foil where occupies 5% by mass in the total mass of the entire copper foil are referred to as the respective external layers, and a region between one external layer and the other external layer is referred to as an internal layer, the internal layer comprises copper as a main element and includes 100 ppm or more of one or mixture of small amount-elements selected from carbon, sulfur, chlorine and nitrogen, and includes zinc at 10% or more in the total mass of zinc included in the entire copper foil. 2 . The copper foil according to claim 1 , wherein a grain size of copper in the internal layer is 1.0 micron-meters or less. 3 . The copper foil according to claim 1 , wherein the external layer of the copper foil has a concentrated zinc-layer higher in zinc content than the rest regions and occupying a part in the external layer. 4 . The copper foil according to claim 1 , wherein a compound composed of zinc and one or mixture of elements selected from carbon, sulfur, chlorine and nitrogen precipitates at a grain boundary of copper in the internal layer. 5 . The copper foil according to claim 1 , wherein a tensile strength is 40 kgf/mm 2 or more. 6 . A negative electrode current collector using a copper foil according to claim 1 . 7 . A negative electrode material of a non-aqueous secondary battery using a negative electrode current collector according to claim 6 .
including at least one metal alloy layer · CPC title
Wires; Strips; Foils · CPC title
Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries · CPC title
Strips or foils · CPC title
Alloys based on zinc · CPC title