Method for manufacturing plated steel sheet having excellent surface quality and press formability, and plated steel sheet manufactured thereby
US-2018345339-A1 · Dec 6, 2018 · US
US12590342B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12590342-B2 |
| Application number | US-202118272628-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 22, 2021 |
| Priority date | Jan 22, 2021 |
| Publication date | Mar 31, 2026 |
| Grant date | Mar 31, 2026 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A hot-pressed member is disclosed including at least one surface that has a filtered centerline waviness Wca of less than or equal to 1.5 μm.
Opening claim text (preview).
The invention claimed is: 1 . A hot-pressed member comprising at least one surface that has a filtered centerline waviness Wca of less than or equal to 1.5 μm, and further comprising a plated layer disposed on the at least one surface, the plated layer having a thickness of 10 to 80 μm, the plated layer having a composition consisting of Al and one or more further elements selected from the group consisting of Si and Mg. 2 . The hot-pressed member according to claim 1 , wherein the at least one surface has a line roughness Ra of less than or equal to 2.0 μm and a skewness Rsk of less than or equal to 0. 3 . A coated member comprising: a base member that comprises the hot-pressed member according to claim 1 ; and a coating layer disposed on at least one surface of the base member and having a thickness of greater than or equal to 15 μm. 4 . A coated member comprising: a base member that comprises the hot-pressed member according to claim 2 ; and a coating layer disposed on at least one surface of the base member and having a thickness of greater than or equal to 15 μm. 5 . A method for manufacturing the hot-pressed member according to claim 1 , the method comprising: heating a steel sheet for hot pressing to a temperature range of an Ac 3 transformation temperature to 1000° C., the steel sheet for hot pressing having at least one surface that has a filtered centerline waviness Wca of less than or equal to 0.75 μm; and subsequently hot-pressing the steel sheet for hot pressing. 6 . A method for manufacturing the coated member according to claim 3 , the method comprising: heating a steel sheet for hot pressing to a temperature range of an Acs transformation temperature to 1000° C., the steel sheet for hot pressing having at least one surface that has a filtered centerline waviness Wca of less than or equal to 0.75 μm; hot-pressing the steel sheet for hot pressing; and subsequently providing a coating layer having a thickness of greater than or equal to 15 μm.
containing more than 50% by weight of zinc · CPC title
Plates; Strips · CPC title
Aluminium or alloys based thereon · CPC title
Zinc or cadmium or alloys based thereon · CPC title
containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur · CPC title