Method for stabilizing wellbore, stabilized wellbore and wellbore stabilizing fluid

US12540268B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-12540268-B2
Application numberUS-202418620446-A
CountryUS
Kind codeB2
Filing dateMar 28, 2024
Priority dateMar 17, 2022
Publication dateFeb 3, 2026
Grant dateFeb 3, 2026

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A method for stabilizing a wellbore includes introducing a hardening agent into the wellbore, mixing the hardening agent with a carrier fluid in the wellbore to produce a wellbore stabilizing fluid, and treating a wellbore wall of the wellbore by contacting the wellbore stabilizing fluid to a surface of the wellbore wall for at least 48 hours. A wellbore stabilizing fluid includes a hardening agent and a carrier fluid. The hardening agent is selected from one of 10 to 100 g/L of the calcium hydroxide nanocrystals, 5 to 99.9% by volume of tetraethyl orthosilicate (TEOS), and 10 to 50 g/L of zinc sulfate. A stabilized wellbore includes a wellbore having a wellbore wall treated with a wellbore stabilizing fluid comprising a hardening agent. The Young's modulus of the treated wellbore wall is at least 5% higher than a Young's modulus of a non-treated wellbore wall.

First claim

Opening claim text (preview).

What is claimed is: 1 . A method for stabilizing a wellbore, the method comprising a treatment cycle of: introducing a hardening agent comprising zinc sulfate into the wellbore; mixing the hardening agent with a carrier fluid in the wellbore to produce a wellbore stabilizing fluid; and treating a wellbore wall of the wellbore by contacting the wellbore stabilizing fluid with a surface of the wellbore wall comprising a formation rock comprising calcium carbonate, and reacting the calcium carbonate comprised in the wellbore wall with the zinc sulfate comprised in the hardening agent to form zinc carbonate on the surface of the wellbore wall, and maintaining the contacting for a duration in a range of from 48 hours to 72 hours. 2 . The method of claim 1 , wherein the hardening agent comprises 10 g/L to 50 g/L of zinc sulfate. 3 . The method of claim 1 , wherein the wellbore stabilizing fluid further comprises a solvent comprising at least one of ethanol and isopropanol. 4 . The method of claim 1 , wherein the method further comprises repeating the treatment cycle of the introducing the hardening agent, the mixing, and the treating. 5 . The method of claim 1 , wherein the method is conducted at an elevated temperature ranging from 40° C. to 100° C. 6 . The method of claim 1 , wherein a Young's modulus of the wellbore wall after the treating is higher than a Young's modulus of the wellbore wall before the treating by 5% to 25.8%. 7 . The method of claim 1 , wherein the wellbore stabilizing fluid further comprises a thickener. 8 . A stabilized wellbore, comprising: a wellbore having a wellbore wall, the wellbore wall: comprising zinc carbonate on a surface, comprising a formation rock comprising calcium carbonate, and treated with a wellbore stabilizing fluid comprising a hardening agent comprising zinc sulfate, wherein: zinc carbonate is formed by reacting the calcium carbonate comprised in the wellbore wall with the zinc sulfate comprised in the hardening agent, and a Young's modulus of the wellbore wall treated with the wellbore stabilizing fluid is higher than a Young's modulus of a wellbore wall of a wellbore not treated by the wellbore stabilizing fluid by 5% to 25.8%. 9 . The stabilized wellbore of claim 8 , wherein the hardening agent comprises 10 g/L to 50 g/L of zinc sulfate. 10 . The stabilized wellbore of claim 8 , wherein the wellbore stabilizing fluid further comprises a thickener.

Assignees

Inventors

Classifications

  • Organic cosolvents · CPC title

  • E21B33/138Primary

    Plastering the borehole wall; Injecting into the formation · CPC title

  • containing organic binders only · CPC title

  • containing silicon · CPC title

  • Hydraulic cements not provided for in one of the groups C04B7/02 - C04B7/34 · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US12540268B2 cover?
A method for stabilizing a wellbore includes introducing a hardening agent into the wellbore, mixing the hardening agent with a carrier fluid in the wellbore to produce a wellbore stabilizing fluid, and treating a wellbore wall of the wellbore by contacting the wellbore stabilizing fluid to a surface of the wellbore wall for at least 48 hours. A wellbore stabilizing fluid includes a hardening a…
Who is the assignee on this patent?
Saudi Arabian Oil Co, Univ King Fahd Pet & Minerals
What technology area does this patent fall under?
Primary CPC classification E21B33/138. Mapped technology areas include Fixed Constructions.
When was this patent published?
Publication date Tue Feb 03 2026 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).