Method for Preparing Positive Electrode Active Material for Lithium Secondary Battery, Positive Electrode Comprising the Positive Electrode Active Material Prepared by the Same and Lithium Secondary Battery
US-2022209231-A1 · Jun 30, 2022 · US
US12506146B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12506146-B2 |
| Application number | US-202118027797-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 13, 2021 |
| Priority date | Sep 25, 2020 |
| Publication date | Dec 23, 2025 |
| Grant date | Dec 23, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing a lithium-nickel complex oxide according to an aspect of the present disclosure comprises: a filling step for filling a firing container with a Ni-containing metal compound and a Li compound to obtain a filling material including the Ni-containing metal compound and the Li compound; and a firing step for firing the filling material that fills the firing container, wherein, in the filling step, when the filling material that fills the firing container is divided into two equal parts in the height direction, the molar ratio A of Li to metals other than Li in the filling material in the upper half region and the molar ratio B of Li to metals other than Li in the filling material in the lower half region satisfy 1<B/A<1.15.
Opening claim text (preview).
The invention claimed is: 1 . A method for manufacturing a lithium-nickel composite oxide, the method comprising: a filling step of filling a firing container with a Ni-containing metal compound and a Li compound to obtain a filling material including the Ni-containing metal compound and the Li compound; and a firing step of firing the filling material filling the firing container, wherein in the filling step, the filling material filling the firing container has an upper half region and a lower half region that are equal in height, and a molar ratio A of Li to metals other than Li in the filling material in the upper half region and a molar ratio B of Li to metals other than Li in the filling material in the lower half region satisfy 1<B/A<1.15. 2 . The method for manufacturing a lithium-nickel composite oxide according to claim 1 , wherein the molar ratio A and the molar ratio B satisfy 1.02≤B/A≤1.12. 3 . The method for manufacturing a lithium-nickel composite oxide according to claim 1 , wherein the Li compound contains lithium hydroxide.
Electric properties · CPC title
containing elements as dopants · CPC title
containing alkali metals, e.g. LiNiO2 · CPC title
Energy storage using batteries · CPC title
Compounds of nickel · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.