Maleimide-based copolymer, method for producing same, and resin composition obtained using same
US-2020369813-A1 · Nov 26, 2020 · US
US12427704B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12427704-B2 |
| Application number | US-202118018000-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 22, 2021 |
| Priority date | Sep 29, 2020 |
| Publication date | Sep 30, 2025 |
| Grant date | Sep 30, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for manufacturing a heat resistant resin composition having superior dispersibility of maleimide-based copolymer, the method including: a melt-kneading step to melt and knead a maleimide-based copolymer (A) and at least one resin (B) selected from the group consisting of ABS resin, ASA resin, AES resin, and SAN resin with an extruder; wherein: a ratio of a melt viscosity of the maleimide-based copolymer (A) with respect to a melt viscosity of the resin (B) obtained with a shear rate of 120/sec and a cylinder temperature of a kneading unit of the extruder is 1.0 or higher and lower than 3.4, is provided.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing a heat resistant resin composition, the method comprising: a melt-kneading step to melt and knead a maleimide-based copolymer (A) and at least one resin (B) selected from the group consisting of ABS resin, ASA resin, AES resin, and SAN resin with an extruder; wherein: a ratio of a melt viscosity of the maleimide-based copolymer (A) with respect to a melt viscosity of the resin (B) obtained with a shear rate of 120/sec and a cylinder temperature of a kneading unit of the extruder is 1.0 or higher and lower than 3.4. 2. The method for manufacturing the heat resistant resin composition of claim 1 , wherein the melt-kneading step is performed under presence of an antioxidant (C). 3. The method for manufacturing the heat resistant resin composition of claim 1 , wherein the extruder is a twin-screw extruder. 4. The method for manufacturing the heat resistant resin composition of claim 3 , wherein a deep groove ratio of a screw of the kneading unit of the twin-screw extruder is 1.55 or higher. 5. The method for manufacturing the heat resistant resin composition of claim 2 , wherein the extruder is a twin-screw extruder. 6. The method for manufacturing the heat resistant resin composition of claim 5 , wherein a deep groove ratio of a screw of the kneading unit of the twin-screw extruder is 1.55 or higher.
containing three or more polymers in a blend · CPC title
Stabilised against heat, light or radiation or oxydation · CPC title
Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors · CPC title
Stabilisers, e.g. against oxydation, light or heat · CPC title