Chemical recycling of waste plastic materials with improved solvolysis catalyst
US-2023203270-A1 · Jun 29, 2023 · US
US12398328B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12398328-B2 |
| Application number | US-202117759459-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 10, 2021 |
| Priority date | Feb 10, 2020 |
| Publication date | Aug 26, 2025 |
| Grant date | Aug 26, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Chemical recycling facilities for processing mixed plastic waste are provided herein. Such facilities have the capability of processing mixed plastic waste streams and utilize a variety of recycling facilities, such as, for example, solvolysis facility, a pyrolysis facility, a cracker facility, a partial oxidation gasification facility, an energy generation/energy production facility, and a solidification facility. Streams from one or more of these individual facilities may be used as feed to one or more of the other facilities, thereby maximizing recovery of valuable chemical components and minimizing unusable waste streams.
Opening claim text (preview).
What is claimed is: 1. A method of processing waste plastic, said method comprising: (a) separating mixed plastic waste (MPW) into a polyethylene terephthalate-enriched (PET-enriched) stream and a polyolefin-enriched (PO-enriched) stream; (b) subjecting at least a portion of said PET-enriched stream to solvolysis in a solvolysis facility to produce a solvolysis effluent, (c) separating the solvolysis effluent to produce an r-terephthalyl product stream, an r-glycol product stream, and one or more of a glycol bottoms coproduct stream or a terephthalyl bottoms coproduct stream; and (d) combining at least a portion of said PO-enriched stream with at least a portion of said glycol bottoms coproduct stream and/or said terephthalyl bottoms coproduct stream to provide a combined stream; and (e) subjecting at least a portion of said combined stream to at least one of (i) partial oxidation (POX) gasification facility; (ii) pyrolysis in a pyrolysis facility; and (iii) chemical conversion in an energy generation facility. 2. The method of claim 1 , wherein said PO-enriched stream comprises not more than 40 weight percent of polyethylene terephthalate, based on a total weight of the PO-enriched stream and wherein said PET-enriched stream comprises not more than 40 weight percent of polyolefin, based on a total weight of the PET-enriched stream. 3. The method of claim 1 , wherein said PET-enriched stream comprises at least 0.1 and not more than 10 weight percent (on a dry basis) of halogens, based on a total weight of said PET-enriched stream. 4. The method of claim 1 , further comprising combining said combined stream with an additional stream to provide a second combined stream and introducing the second combined stream into at least one of (i) through (iii). 5. The method of claim 4 , wherein said additional stream originates from at least one of said pyrolysis facility, a solidification facility, or a cracking facility. 6. The method of claim 1 , wherein at least a portion of said PO-enriched stream is introduced into said POX gasification facility. 7. The method of claim 1 , wherein step (d) includes subjecting at least a portion of said combined stream to two or more of (i) through (iii). 8. The method of claim 1 , wherein said MPW comprises; PVC in an amount of at least 0.001 and/or not more than 5 weight percent, at least 0.1 and/or not more than 25 weight percent of non-plastic solids, at least 5 weight percent PET, and at least 5 weight percent PO, each based on a total weight of said MPW. 9. The method of claim 1 , wherein said PO-enriched stream comprises at least 50 weight percent polyolefin (PO) and has one or more of the following characteristics (i) through (vii) (i) an ash content of not more than about 5 weight percent; (ii) a halogen content of not more than 250 ppm by weight (on a dry basis); (iii) not more than 5 weight percent of nitrogen-containing compounds; (iv) not more than 10 weight percent of polyethylene terephthalate; (v) a mercury content of not more than 1 ppm; (vi) an arsenic content of not more than 100 ppm; and (vii) a melt viscosity of less than 25,000 poise measured at 10 rad/s and 250° C. 10. The method of claim 9 , wherein said MPW comprises at least 0.1 and/or not more than 25 weight percent of non-plastic solids, based on a total weight of said MPW. 11. The method of claim 9 , wherein said PO-enriched stream comprises two of said characteristics (i) through (vii). 12. The method of claim 1 , wherein said solvolysis facility comprises a methanolysis facility. 13. The method of claim 1 , wherein at least a portion of at least one of said glycol bottoms coproduct stream or said terephthalyl bottoms coproduct stream is introduced into said (i) POX gasification facility.
Chemical treatment, e.g. pH adjustment or oxidation (involving an extraction step B09B3/80) · CPC title
containing hydroxyl groups · CPC title
Feed preparation · CPC title
Recovery or working-up of waste materials (recovery of plastics B29B17/00; polymerisation processes involving purification or recycling of waste polymers or their depolymerisation products C08B, C08C, C08F, C08G, C08H) · CPC title