Novel vinyl silane compound
US-2018334467-A1 · Nov 22, 2018 · US
US12359040B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12359040-B2 |
| Application number | US-202017758285-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 21, 2020 |
| Priority date | Dec 31, 2019 |
| Publication date | Jul 15, 2025 |
| Grant date | Jul 15, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A vulcanizing agent is added during the processing of a polymer, and can form a crosslinking structure network in the polymer, thereby improving the mechanical properties of the material. Furthermore, the crosslinking agent can also de-crosslink the polymer material at a high temperature, and after being cooled, same can be crosslinked again to produce a network structure, thus endowing the polymer material with thermoplasticity for repeated processing.
Opening claim text (preview).
The invention claimed is: 1. A vulcanizing agent, comprising a compound selected from 2. A method for vulcanizing a polymer, comprising forming a mixture comprising a polymer, an initiator, a heat stabilizer, and the vulcanizing agent of claim 1 ; and heating the mixture to form a vulcanized polymer. 3. A method according to claim 2 , wherein a mass ratio of the polymer to the vulcanizing agent is 100:0.01 to 100:10, a mass ratio of the polymer to the initiator is 100:0.01 to 100:1, and a mass ratio of the polymer to the heat stabilizer is 100:0 to 100:1. 4. The method according to claim 3 , wherein the polymer is selected from at least one of polyolefin resins and polyolefin rubbers. 5. The method according to claim 3 , wherein the initiator is selected from organic peroxides and azo initiators. 6. The method according to claim 3 , wherein the heat stabilizer is selected from at least one of hindered phenolic macromolecular antioxidants, phosphite antioxidants, and alkyl ester antioxidants. 7. The method according to claim 3 , further comprising: feeding the mixture into a reactive processing equipment to react at a temperature above 120° C.; and extruding the heated mixture from the reactive processing equipment to form a product; and cooling the product to allow crosslinking within the product. 8. The method according to claim 7 , wherein the reactive processing equipment is single-screw extruder, twin-screw extruder, open mill, or internal mixer.
containing no other elements than carbon or hydrogen · CPC title
having one oxygen atom in the ring · CPC title
Peroxides · CPC title
Propene · CPC title
PP, i.e. polypropylene · CPC title