A method of treating silicon carbide fibers
US-2018194686-A1 · Jul 12, 2018 · US
US12338181B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12338181-B2 |
| Application number | US-202218571551-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 20, 2022 |
| Priority date | Jun 23, 2021 |
| Publication date | Jun 24, 2025 |
| Grant date | Jun 24, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for treating at least one silicon carbide fibre includes a surface layer including carbon and/or a silicon oxycarbide, the treatment including at least removing the surface layer from the fibre by placing in contact with an ammonia phase in the supercritical state.
Opening claim text (preview).
The invention claimed is: 1. A method for treating at least one silicon carbide fibre comprising a surface layer containing carbon and/or a silicon oxycarbide, the method comprising at least removing the surface layer from the fibre by placing it in contact with an ammonia phase in the supercritical state. 2. The method according to claim 1 , wherein the removal of the surface layer is carried out in a treatment chamber, and wherein the method further comprises, after the removal, forming a coating on said at least one fibre, in the treatment chamber, from a treatment medium comprising at least ammonia. 3. The method according to claim 1 , wherein a temperature of the ammonia phase is greater than or equal to 600° C. 4. The method according to claim 3 , wherein the temperature of the ammonia phase is between 800° C. and 1200° C., and a pressure of the ammonia phase is between 100 bar and 150 bar. 5. The method according to claim 1 , wherein said at least one fibre is heated by microwaves during the treatment. 6. The method according to claim 1 , wherein said at least one fibre-moves through a treatment chamber during the treatment. 7. The method according to claim 1 , wherein said at least one fibre is made of silicon carbide having an oxygen content less than or equal to 1% in atomic percent. 8. A method for manufacturing a composite material part, comprising: treating fibers of a fibrous reinforcement by implementing a method according to claim 1 , and forming a matrix in the pores of the fibrous reinforcement.
Silicon carbide · CPC title
Wet etching, e.g. with etchants dissolved in organic solvents · CPC title
Heat treatment · CPC title
Nitrides · CPC title
characterised by the material treated · CPC title