Catalyst for fluidized catalytic cracking and method for fluidized catalytic cracking
US-2015375218-A1 · Dec 31, 2015 · US
US12337299B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12337299-B2 |
| Application number | US-202117608333-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 15, 2021 |
| Priority date | Jan 16, 2020 |
| Publication date | Jun 24, 2025 |
| Grant date | Jun 24, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for using a natural attapulgite is disclosed. The method includes using the natural attapulgite as a natural nano mineral enzyme. The results of the examples show that the natural attapulgite has peroxidase-like activity, catalase-like activity or superoxide dismutase-like activity, and good biocompatibility. Compared with protease, the natural attapulgite has the advantages such as large reserves, easy to obtain, low cost, high temperature resistance and wide range of pH value. Compared with a developed artificial nano enzymes, the natural attapulgite further has the advantages such as multi-function, natural non-toxic (from nature, no heavy metals), good biocompatibility, easy to obtain, no complex processing, and huge surface area which provides a place for cell growth and proliferation.
Opening claim text (preview).
What is claimed is: 1. A method for using a natural attapulgite comprising: mixing a natural attapulgite dispersion, an H 2 O 2 solution, a substrate solution and a buffer solution to obtain a mixture, and subjecting the mixture to enzyme catalysis; wherein the natural attapulgite dispersion consists of the natural attapulgite and water, and the natural attapulgite dispersion has a concentration of the natural attapulgite of 1-5 mg/mL; and the natural attapulgite is a one-dimensional fibrous hydrated magnesium aluminosilicate clay mineral. 2. The method of claim 1 , wherein the buffer solution is HAc-NaAc or a phosphate buffer solution, and has a pH value of 2-10. 3. The method of claim 1 , wherein the H 2 O 2 solution has a mass concentration of 30%. 4. The method of claim 1 , wherein the buffer solution has a concentration of 0.1 M and a pH value of 7.0. 5. A method for using a natural attapulgite comprising: adding 0.4 mL of a natural attapulgite dispersion with a concentration of 2.5 mg/mL into 5.0 mL of a buffer solution, and adding 100 μL of an H 2 O 2 solution thereto, and measuring a solubility of O 2 produced at different reaction time; wherein the natural attapulgite dispersion consists of the natural attapulgite and water; and the natural attapulgite is a one-dimensional fibrous hydrated magnesium aluminosilicate clay mineral.
in a liquid or molten state · CPC title
Water · CPC title
of ultrasonic wave energy · CPC title
Grinding · CPC title
100-500 m2/g · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.