Aluminum member and method for producing same
US-2020299811-A1 · Sep 24, 2020 · US
US12168835B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12168835-B2 |
| Application number | US-202117332779-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 27, 2021 |
| Priority date | Nov 30, 2018 |
| Publication date | Dec 17, 2024 |
| Grant date | Dec 17, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
An example aluminum member consisting of a mother material containing aluminum or an aluminum alloy, and an anodic oxide film on the surface of the mother material, in which the arithmetical mean roughness Ra, the mean length of roughness curve elements RSm, and the Hunter whiteness of the aluminum member, measured from the surface side of the anodic oxide film, are 0.1 μm or more, 10 μm or less, and 60 to 90, respectively.
Opening claim text (preview).
What is claimed is: 1. An aluminum member consisting of: a mother material containing aluminum or an aluminum alloy; and an anodic oxide film on a surface of the mother material, wherein a thickness of the anodic oxide film is 6 to 100 μm, wherein an arithmetical mean roughness Ra, a mean length of roughness curve elements RSm, and a Hunter whiteness of the aluminum member, measured from a surface side of the anodic oxide film, are 0.1 μm or more, 10 μm or less, and 60 to 90, respectively, wherein the surface side of the anodic oxide film is opposite a side of the anodic oxide film on the surface of the mother material. 2. The aluminum member according to claim 1 , wherein a relational expression between the arithmetical mean roughness Ra and the mean length of roughness curve elements RSm satisfies 0.1≤Ra/RSm≤1.2, and the Hunter whiteness of the aluminum member, measured from the surface side of the anodic oxide film, is 70 to 90.
all layers being formed of aluminium or aluminium alloys · CPC title
characterised by the electrolytes used · CPC title
containing organic acids · CPC title
Producing integrally coloured layers · CPC title
Pretreatment {, e.g. desmutting} · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.