Magnetic core and coil component using same
US-2016336104-A1 · Nov 17, 2016 · US
US12146208B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12146208-B2 |
| Application number | US-202117313438-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 6, 2021 |
| Priority date | Sep 12, 2012 |
| Publication date | Nov 19, 2024 |
| Grant date | Nov 19, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Raw material powder containing iron powder, copper powder, and tin powder is compressed to form a green compact. The green compact is sintered in a temperature range of from 750 to 900° C., to bond iron structures to each other with copper and tin.
Opening claim text (preview).
The invention claimed is: 1. A method of manufacturing a machine part, the method comprising the steps of: compressing raw material powder containing 1 to 10 wt % of copper powder, 0.5 to 2 wt % of tin powder, and 0.1 wt % or more and less than 0.5 wt % of graphite powder, with the balance being iron powder to form green compacts; and sintering the green compacts in a temperature range of 750° C. or more and less than 900° C. in a non-aligned state in which directions and postures of the green compacts are not uniformized, to bond iron structures to each other with copper and tin and obtain sintered compacts, wherein the sintered compacts are not subjected further sintering. 2. The method of manufacturing of the machine part according to claim 1 , wherein the iron structures are bonded to each other with a copper-tin alloy. 3. The method of manufacturing of the machine part according to claim 1 , wherein the iron-based sintered metal comprises free graphite. 4. The method of manufacturing of the machine part according to claim 1 , wherein the raw material powder has a blending ratio of tin to copper of 1/5 or more and 1 or less in terms of weight ratio. 5. The method of manufacturing of the machine part according to claim 1 , wherein the temperature range for sintering the green compacts is from 800 to 850° C.
Camshafts · CPC title
Manufacture of workpieces or articles from metallic powder characterised by the special shape of the product · CPC title
Both compacting and sintering (by forging B22F3/17) · CPC title
containing inorganic lubricating or binding agents, e.g. metal salts · CPC title
Tools for producing, mounting or adjusting, e.g. some part of the distribution · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.