Substrate for flexible device
US-11414762-B2 · Aug 16, 2022 · US
US12144239B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12144239-B2 |
| Application number | US-201917274030-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 29, 2019 |
| Priority date | Sep 12, 2018 |
| Publication date | Nov 12, 2024 |
| Grant date | Nov 12, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A substrate for flexible device, including a stainless steel sheet, an oxide layer formed on a surface of the stainless steel sheet, and a glass layer of electrically-insulating bismuth-based glass formed in a form of layer on the surface of the oxide layer. Also disclosed is a sheet for flexible device, including a stainless steel sheet, and an oxide layer on a surface of the stainless steel sheet, the oxide layer having a thickness of not less than 30 nm.
Opening claim text (preview).
The invention claimed is: 1. A substrate for flexible device, including a stainless steel sheet, an oxide layer on a surface of the stainless steel sheet, and a glass layer of electrically-insulating bismuth-based glass in a form of layer on a surface of the oxide layer, wherein a chromium concentration at a point distanced by 20 nm in a thickness direction of the oxide layer from an interface between the oxide layer and the glass layer is not less than 30 atomic %. 2. The substrate for flexible device according to claim 1 , wherein the oxide layer has a thickness of not less than 30 nm. 3. The substrate for flexible device according to claim 1 , wherein the oxide layer has a thickness of not less than 80 nm. 4. The substrate for flexible device according to claim 1 , wherein the chromium concentration at the point distanced by 20 nm in the thickness direction of the oxide layer from the interface between the oxide layer and the glass layer is not less than 50 atomic %. 5. The substrate for flexible device according to claim 1 , wherein the bismuth-based glass contains Bi 2 O 3 , ZnO and B 2 O 3 .
Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension · CPC title
Oxide of transition metal or Al · CPC title
Coating layer not in excess of 5 mils thick or equivalent · CPC title
Absolute thicknesses specified · CPC title
Film [e.g., glaze, etc.] · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.