Composite article
US-10611929-B2 · Apr 7, 2020 · US
US12090737B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12090737-B2 |
| Application number | US-201917274632-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 11, 2019 |
| Priority date | Sep 14, 2018 |
| Publication date | Sep 17, 2024 |
| Grant date | Sep 17, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Described herein is a laminate including at least one first layer of at least one first metal and at least one further layer of a polymer composition (PC). Also described herein is a process for producing the laminate.
Opening claim text (preview).
The invention claimed is: 1. A laminate comprising at least one first layer of at least one first metal and at least one further layer of a polymer composition (PC), wherein the polymer composition (PC) comprises the following components: (A) 55% to 85% by weight of at least one polyamide selected from the group consisting of PA 6, PA 6.6, PA 6.10, PA 6.12, PA 12, PA 6.36, PA 6/6.6, PA 6/6I6T, PA 6/6I, PA 6/6.36 and PA 6/6T, (B) 5% to 20% by weight of at least one first copolymer obtainable by polymerizing at least the following components: (B1) at least one first C 2 -C 20 -alkene selected from the group consisting of ethene, propene, 1-butene, 2-butene, octene and butadiene, (B2) at least one second C 2 -C 20 -alkene selected from the group consisting of ethene, propene, 1-butene, 2-butene, octene and butadiene, and (B4) maleic anhydride, wherein components (B1) and (B2) are different than one another, and (C) 10% to 30% by weight of at least one second copolymer obtainable by polymerizing at least the following components: (C1) at least one third C 2 -C 20 -alkene selected from the group consisting of ethene, propene, 1-butene, 2-butene, octene and butadiene, and (C2) at least one acrylic acid derivative selected from the group consisting of methyl acrylate, butyl acrylate and acrylic acid; wherein the laminate has a peel strength of at least 460 N/40 m for a peel test according to ASTM D1876. 2. The laminate according to claim 1 , wherein the laminate additionally comprises at least one second layer of at least one second metal and wherein the at least one first layer is joined to the at least one second layer via the at least one further layer. 3. The laminate according to claim 1 , wherein the at least one first metal is selected from the group consisting of iron, aluminum, copper, nickel and magnesium and also alloys thereof. 4. The laminate according to claim 1 , wherein the at least one first layer has a thickness in the range from 0.1 mm to 0.6 mm and/or wherein the at least one further layer has a thickness in the range from 0.02 to 2 mm. 5. A process for producing a laminate according to claim 1 , comprising the steps of a) providing a film of a polymer composition (PC) comprising the following components: (A) at least one polyamide, (B) at least one first copolymer obtainable by polymerizing at least the following components: (B1) at least one first C 2 -C 20 -alkene and (B2) at least one second C 2 -C 20 -alkene, where components (B1) and (B2) are different than one another, and (C) at least one second copolymer obtainable by polymerizing at least the following components: (C1) at least one third C 2 -C 20 -alkene and (C2) at least one acrylic acid derivative, b) heating a first sheet of at least one first metal, and c) pressing the heated first sheet from step b) with the film provided in step a) to obtain the laminate. 6. The process according to claim 5 , wherein step b) comprises heating the first sheet to a temperature in the range from 150° C. to 350° C. 7. The process according to claim 5 , wherein the heating of the first sheet in step b) is effected by inductive means. 8. The process according to claim 5 , wherein step a) comprises providing the film by an extrusion process.
Dimensional properties · CPC title
characterised by the heating method · CPC title
comprising acrylic (co)polymers · CPC title
comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)} · CPC title