Casting mold of grading with silicon carbide
US-2015352630-A1 · Dec 10, 2015 · US
US12090545B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12090545-B2 |
| Application number | US-202318198039-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 16, 2023 |
| Priority date | May 30, 2022 |
| Publication date | Sep 17, 2024 |
| Grant date | Sep 17, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A riser tube coating for a cast aluminum alloy includes a coating-riser tube contact layer material and a coating-aluminum liquid contact layer material. The present invention has a coating protection effect to the maximum mainly by designing ratios of ZrO, Al2O3, ZnO, binders and other materials and a coat drying heat treatment process, and finally realizes effects of protecting a riser tube, being free of aluminum sticking and prolonging a service life.
Opening claim text (preview).
What is claimed is: 1. A riser tube coating for a cast aluminum alloy, characterized by comprising a coating-riser tube contact layer material and a coating-aluminum liquid contact layer material, wherein the coating-riser tube contact layer material comprises ZrO 2 , Al 2 O 3 , ZnO and a binder, ZrO 2 accounts for 70%-80%, Al 2 O 3 accounts for 10%-15%, ZnO accounts for 10%-15%, and a weight ratio of the binder to the materials is 10:1; and the coating-aluminum liquid contact layer material is mainly ZrO 2 , Al 2 O 3 , ZnO and a binder, in the coating-aluminum liquid contact layer material, the ZrO 2 accounts for 80%-90%, Al 2 O 3 accounts for 5%-10%, ZnO accounts for 5%-10%, and a weight ratio of the binder to the materials is 15:1. 2. The riser tube coating for the cast aluminum alloy according to claim 1 , characterized in that ZrO 2 in the coating-riser tube contact layer material is of a particle structure, a particle size is 50 μm-70 μm, Al 2 O 3 is of a particle structure, a particle size is 40 μm-60 μm, ZnO is of a particle structure, and a particle size is 40 μm-60 μm. 3. The riser tube coating for the cast aluminum alloy according to claim 2 , characterized in that a thickness of the coating-riser tube contact layer material is 0.5 mm-1.0 mm. 4. The riser tube coating for the cast aluminum alloy according to claim 1 , characterized in that ZrO 2 in the coating-aluminum liquid contact layer material is of a particle structure, a particle size is 30 μm-50 μm, Al 2 O 3 is of a particle structure, a particle size is 20 μm-30 μm, ZnO is of a particle structure, and a particle size is 20 μm-30 μm. 5. The riser tube coating for the cast aluminum alloy according to claim 4 , characterized in that a thickness of the coating-aluminum liquid contact layer material is 1.0 mm-1.5 mm.
Features with respect to supply of molten metal, e.g. ingates, circular gates, skim gates · CPC title
Low pressure casting, i.e. making use of pressures up to a few bars to fill the mould · CPC title
Filters · CPC title
Selection of compositions for coating the surfaces of moulds, cores, or patterns · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.