Method of producing electrode for secondary battery, electrode, and secondary battery including electrode
US-2022293904-A1 · Sep 15, 2022 · US
US12080870B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12080870-B2 |
| Application number | US-202217692191-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 11, 2022 |
| Priority date | Mar 12, 2021 |
| Publication date | Sep 3, 2024 |
| Grant date | Sep 3, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of producing an electrode disclosed here includes a step in which a moisture powder formed of agglomerated particles; a step in which by using the moisture powder, a coating film composed of the moisture powder is formed on an electrode current collector, with a gas phase of the coating film being remained so that the average film thickness of the coating film is 50 μm or more; a step in which the coating film on the current collector is transported, concavo-convex transfer is performed using a roll mold, and thus at least one groove extending in the transport direction is formed in a center of a surface part of the coating film, with the groove being formed to have a depth satisfying ( 9/10×t 1 )>t 2 ; and a step in which the coating film formed on the current collector is dried to form an electrode active material layer.
Opening claim text (preview).
What is claimed is: 1. A method of producing an electrode for a secondary battery having any electrode current collector of positive and negative electrodes and an electrode active material layer, the method comprising: a step in which a moisture powder formed of agglomerated particles containing at least an electrode active material, a binder resin, and a solvent is prepared, with a solid phase, a liquid phase, and a gas phase in at least 50 number % or more of the agglomerated particles forming a pendular state or a funicular state in the moisture powder; a step in which by using the moisture powder, a coating film composed of the moisture powder is formed on the electrode current collector, with a gas phase of the coating film being remained, and with an average film thickness t 1 (μm) of the coating film being 50 μm or more; a step in which the coating film on the electrode current collector is transported, concavo-convex transfer is performed using a roll mold, and thus at least one groove extending in a transport direction is formed in a center of a surface part of the coating film, with the groove being formed to have a depth t 2 (μm) satisfying ( 9/10×t 1 )>t 2 ; and a step in which the coating film formed on the electrode current collector is dried to form an electrode active material layer. 2. The method of producing an electrode for a secondary battery according to claim 1 , wherein, in the moisture powder prepared in the step in which the moisture powder is prepared, when a bulk specific gravity measured by putting a moisture powder (g) into a container having a predetermined volume (mL) with leveling and without applying a force is set as a loose bulk specific gravity X (g/mL), and a specific gravity calculated from the composition of the moisture powder assuming that there is no gas phase is set as a true specific gravity Y (g/mL), a ratio: Y/X of the true specific gravity Y to the loose bulk specific gravity X is 1.2 or more. 3. The method of producing an electrode for a secondary battery according to claim 1 , wherein, in the step in which the at least one groove extending in the transport direction is formed, the at least one groove is formed in plurality on the coating film. 4. The method of producing an electrode for a secondary battery according to claim 3 , wherein, in the step in which the at least one groove extending in the transport direction is formed, a groove present in a central part in a width direction is formed to be deeper than a groove present at an end of the coating film in a width direction orthogonal to the transport direction.
Physical characteristics, e.g. porosity, surface area · CPC title
by coating on electrode collectors · CPC title
Energy storage using batteries · CPC title
Batteries, accumulators or fuel cells (battery cases B29L2031/7146) · CPC title