Thermoplastic resin film, its manufacturing method, and laminated body
US-2019055393-A1 · Feb 21, 2019 · US
US12030281B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12030281-B2 |
| Application number | US-202017598357-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 11, 2020 |
| Priority date | Mar 29, 2019 |
| Publication date | Jul 9, 2024 |
| Grant date | Jul 9, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of manufacturing a glass resin laminated body includes a step of sticking a glass film on a resin film via an adhesive layer while holding the glass film and the resin film between a first roller that presses against the resin film and a second roller that is disposed opposite to the first roller and that presses against the glass film. A ratio of an elastic modulus P 1 of a surface layer of the first roller to an elastic modulus P 2 of the resin film P 1 /P 2 satisfies a relation of 3×10 −3 ≤P 1 /P 2 ≤1.0.
Opening claim text (preview).
The invention claimed is: 1. A method of manufacturing a glass resin laminated body comprising: a step of sticking a glass film on a resin film via an adhesive layer while holding the glass film and resin film between a first roller that presses against the resin film and a second roller that is disposed opposite to the first roller and that presses against the glass film, wherein a thickness of the adhesive layer is less than or equal to 5 μm, a ratio of an elastic modulus P 1 of a surface layer of the first roller to an elastic modulus P 2 of the resin film P 1 /P 2 satisfies a relation of 3×10 −3 ≤P 1 /P 2 ≤1.0, the surface layer of the first roller is formed of a material having an elastic modulus that is lower than the elastic modulus of iron, the surface layer of the first roller is a portion of the first roller 1 mm inward from a surface of the first roller towards a center; and the surface layer of the first roller is formed of a resin from a group consisting of polyethylene terephthalate, polyethylene, or polypropylene. 2. The method of manufacturing a glass resin laminating body according to claim 1 , wherein the resin film includes a polarizing plate disposed on an opposite side of the adhesive layer with respect to the glass film. 3. The method of manufacturing a glass resin laminating body according to claim 2 , wherein the polarizing plate includes a polarizer and a protection film.
characterised by the pressing technique, e.g. using action of vacuum or fluid pressure · CPC title
characterised by using adhesives · CPC title
Displays, e.g. liquid crystal displays, plasma displays · CPC title
Polarizing, birefringent, filtering · CPC title
5 or more layers · CPC title