Electrode sheet for all-solid state secondary battery, all-solid state secondary battery, and method of manufacturing electrode sheet for all-solid state secondary battery and all-solid state secondary battery
US-2020313161-A1 · Oct 1, 2020 · US
US12021243B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12021243-B2 |
| Application number | US-202117375519-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 14, 2021 |
| Priority date | Jul 16, 2020 |
| Publication date | Jun 25, 2024 |
| Grant date | Jun 25, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a sulfide all-solid battery having an anode current collector of powerful adhesiveness which is difficult to be sulfurized. The sulfide all-solid-state battery including: a cathode layer; an anode layer; and a sulfide solid electrolyte layer disposed between the cathode layer and the anode layer, wherein the anode layer has an anode mixture layer, and an anode current collector on a face of the anode mixture layer, the face being on an opposite side of the sulfide solid electrolyte layer, the anode current collector is electrolytic iron foil that does not substantially contain other elements, and the anode current collector has surface roughness Ra of 0.2 μm to 0.6 μm, and surface roughness Rz of 2 μm to 6 μm.
Opening claim text (preview).
What is claimed is: 1. A sulfide all-solid-state battery comprising: a cathode layer; an anode layer; and a sulfide solid electrolyte layer disposed between the cathode layer and the anode layer, wherein the anode layer has an anode mixture layer, and an anode current collector on a face of the anode mixture layer, the face being on an opposite side of the sulfide solid electrolyte layer, the anode current collector is an electrolytic iron foil that does not substantially contain other elements, the anode current collector has surface roughness Ra of 0.2 μm to 0.6 μm, and surface roughness Rz of 2 μm to 6 μm, and the anode current collector has surface Martens hardness of 1090 N/mm 2 to 2820 N/mm 2 . 2. The sulfide all-solid-state battery according to claim 1 , wherein an elongation percentage of the anode current collector is 5% to 12%. 3. The sulfide all-solid-state battery according to claim 1 , wherein the anode current collector has surface Martens hardness of 1090 N/mm 2 _to 2050 N/mm .
Solid materials · CPC title
in the form of mixed materials (H01M4/668 takes precedence) · CPC title
as mixtures · CPC title
Manufacturing or production processes characterised by the final manufactured product · CPC title
Energy storage using batteries · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.