Perovskite solar battery and tandem solar battery including same
US-2020176618-A1 · Jun 4, 2020 · US
US12014885B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12014885-B2 |
| Application number | US-201916393111-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 24, 2019 |
| Priority date | Apr 24, 2018 |
| Publication date | Jun 18, 2024 |
| Grant date | Jun 18, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of forming a photoactive device includes steps of: forming a photoactive layer, the photoactive layer comprising a perovskite material and a dopant; wherein the photoactive device comprises a positive electrode and a negative electrode; wherein said photoactive layer is directly or indirectly in electronic communication with the positive electrode and directly or indirectly in electronic communication with the negative electrode; and wherein the photoactive device is free of a hole transport layer between the photoactive layer and the positive electrode.
Opening claim text (preview).
The invention claimed is: 1. A method of forming a photoactive device containing a single photoactive layer, the method comprising steps of: forming the single photoactive layer, the photoactive layer comprising a perovskite material and a dopant; wherein the step of forming comprises coating a perovskite-dopant solution onto a receiving surface of a substrate; wherein the perovskite-dopant solution comprises at least a perovskite ink and a dopant; wherein the perovskite-dopant solution comprises one or more additives; wherein the photoactive layer comprises crystalline grains characterized by an average physical dimension selected from the range of 1000 nm to 2000 nm; wherein a concentration of the dopant in the photoactive layer is selected from the range of 0.01 wt. % to 0.05 wt. %; wherein the dopant is a p-type dopant; wherein the one or more additives comprise methylammonium hypophosphite (MHP) having a concentration in the solution selected from the range of 0.01 wt. % to 10 wt. %.; wherein the step of forming comprises doping the perovskite material with the dopant by solid diffusion; wherein doping by solid diffusion comprises providing a perovskite material free of the dopant in proximity with a solid dopant material and allowing the solid dopant material to diffuse into the perovskite material; wherein the photoactive device comprises a positive electrode and a negative electrode; wherein said photoactive layer is in electronic communication with the positive electrode and in electronic communication with the negative electrode; wherein the photoactive device is free of a hole transport layer between the photoactive layer and the positive electrode; wherein the photoactive device comprises an electron transport layer between the photoactive layer and the negative electrode; and wherein the photoactive device does not contain multiple photoactive layers, and the single photoactive layer is in contact with the electron transport layer. 2. The method of claim 1 , comprising preparing the perovskite-dopant solution by combining at least: the perovskite ink, the dopant, and one or more solvents. 3. The method of claim 1 , the step of coating comprising doctor blading. 4. The method of claim 1 , wherein at least a portion of the photoactive layer is in direct physical contact with the positive electrode. 5. The method of claim 1 , wherein at least one of the substrate and the receiving surface of the substrate is at least a portion of the positive electrode. 6. The method of claim 1 , wherein the dopant comprises 2,3,5,6-tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ). 7. The method of claim 1 , wherein the positive electrode is a transparent electrical conductor. 8. The method of claim 1 , wherein a total concentration of the one or more additives in the perovskite-dopant solution is selected from the range of 0.075 wt. % to 0.8 wt. %. 9. The method of claim 1 , wherein the perovskite material is characterized by a chemical formula comprising at least two chemical species selected from the group consisting of Pb, Sn, Sb, Fe, Ge, Mn, Mo, Ta, Ag, Na, K, Ru, Cs, formamidinium (“FA”), methylammonium (“MA”), ethylammonium, propylammonium, butylammonium, amylammonium, hexylammonium, heptylammonium, octylammonium, oleylammonium, formamidinium, dodecylammonium, phenylethylammonium, benzylammonium, ethylenediammonium, tetramethylammonium, tetraethylammonium, tetrabutylammonium, hexadecyl trimethyl ammonium, and ethanediammonium, and at least one chemical species selected from the group consisting of I, Br, Cl, F, COO, BF3 and SCN. 10. The method of claim 1 , wherein the photoactive device is a photovoltaic cell. 11. The method of claim 10 , wherein an average photovoltaic efficiency of the photoactive device is greater by a factor of 1.8 to 2.2 times than an average photovoltaic efficiency of an otherwise equivalent photovoltaic cell free of the dopant. 12. The method of claim 1 , wherein the photoactive device is free of an undoped perovskite layer. 13. The method of claim 1 , wherein the positive electrode is in contact with the photoactive layer, the photoactive layer is in contact with the electron transport layer, and the electron transport layer is in contact with the negative electrode. 14. The method of claim 1 , wherein the electron transport layer comprises C 60 and/or bathocuproine. 15. The method of claim 1 , wherein a total concentration of the one or more additives in the perovskite-dopant solution is selected from the range of 0.225 wt. % to 1 wt. %. 16. The method of claim 1 , wherein the dopant comprises 2,3,5,6-tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ) and wherein the one or more additives comprise methylammonium hypophosphite (MHP). 17. The method of claim 1 , wherein a total concentration of the one or more additives in the perovskite-dopant solution is selected from the range of 0.01 wt. % to 0.35 wt. %.
Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3 · CPC title
Photovoltaic [PV] devices · CPC title
comprising an organic dye as the active light absorbing material, e.g. adsorbed on an electrode or dissolved in solution · CPC title
comprising organic-organic junctions, e.g. donor-acceptor junctions · CPC title
Doping active layers, e.g. electron transporting layers · CPC title