Anode active material, anode comprising the same, secondary battery comprising the anode, and method for preparing the same
US-2024250240-A1 · Jul 25, 2024 · US
US11981575B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11981575-B2 |
| Application number | US-201917295057-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 5, 2019 |
| Priority date | Mar 5, 2019 |
| Publication date | May 14, 2024 |
| Grant date | May 14, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Silicon and silica values are obtained from recycled organosilicon products such as silicones, by introducing a recycle feed containing the organosilicon products into an electric furnace while producing metallurgical grade silicon from a silica source and a carbon source.
Opening claim text (preview).
The invention claimed is: 1. A process for producing metallurgical silicon, comprising: reacting in an electric furnace, a mixture comprising: a raw material mixture containing silicon dioxide and carbon, and a recycle feed containing organosilicon compounds, and recovering metallurgical grade silicon. 2. The process of claim 1 , wherein the recycle feed contains at least 50% by weight of organosilicon compounds. 3. The process of claim 1 , wherein the recycle feed is a particle mixture whose particle size parameter d 50 is at least 1 mm. 4. The process of claim 1 , wherein the silicon dioxide in the raw material mixture comprises quartz and/or quartzite. 5. The process of claim 1 , wherein the carbon in the raw material mixture comprises coke, petroleum coke, bituminous coke, charcoal, wood particles, or mixtures thereof. 6. The process of claim 1 , wherein the proportion of the recycle feed based on the sum of the raw material mixture and the recycle feed is not more than 20% by weight.
with carbon or a solid carbonaceous material, i.e. carbo-thermal process · CPC title