High Flow Automotive Exterior Compounds with Excellent Surface Appearance
US-2019241726-A1 · Aug 8, 2019 · US
US11970602B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11970602-B2 |
| Application number | US-201816969972-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 14, 2018 |
| Priority date | Feb 14, 2018 |
| Publication date | Apr 30, 2024 |
| Grant date | Apr 30, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A first composition comprising a first ethylene/α-olefin/diene interpolymer and a second ethylene/α-olefin interpolymer, and wherein the first composition comprises from 0.1 to 1.0 wt % diene, based on the weight of the first composition, and wherein the first composition comprises from 40 to 70 wt % ethylene, based on the weight of the first composition.
Opening claim text (preview).
What is claimed is: 1. A first composition comprising from 30 to 40 wt % of a first ethylene/α-olefin/diene interpolymer and from 60 to 70 wt % of a second ethylene/α-olefin interpolymer, and wherein the first composition comprises from 0.1 to 1.0 wt % diene, based on the weight of the first composition, and wherein the first composition comprises from 45 to 65 wt % ethylene, based on the weight of the first composition, and wherein the first ethylene/α-olefin/diene interpolymer has a weight average molecular weight (Mw) from 250,000 to 500,000 g/mole, and a diene content from 0.40 to 0.60 wt % and has a C2 (polymerized ethylene) content from 55 to 80 wt %, based on the weight of the first ethylene/α-olefin/diene interpolymer, and wherein the first composition has a weight average molecular weight (Mw) from 200,000 to 280,000 g/mole, a % crystallinity from 0.5% to 12% and has a “% Peak Area (21.3 to 22.0 ppm)” >5.0%, as determined by 13C NMR and the ratio of the C2 (polymerized ethylene) content of the first composition to the C2 (polymerized ethylene) content in the first ethylene/α-olefin/diene interpolymer is from 0.50 to 1.10; and wherein the ratio of the Mooney Viscosity (ML, 1+4, 125° C.) of the first composition to the Mooney Viscosity (ML, 1+4, 125° C.) of the first ethylene/α-olefin/diene interpolymer is from 0.75 to 1.05. 2. The first composition of claim 1 , wherein the first ethylene/α-olefin/diene interpolymer and the second ethylene/α-olefin interpolymer are each, independently, an EPDM. 3. The first composition of claim 1 , wherein the first composition has a molecular weight distribution (Mw/Mn) from 2.10 to 3.20. 4. The first composition of claim 1 , wherein the first interpolymer and the second interpolymer comprise ≥95 wt % of the total weight of the first composition. 5. A crosslinked composition comprising the first composition of claim 1 . 6. An article comprising at least one component formed from the first composition of claim 1 . 7. A composition comprising the first composition of claim 1 and an additive. 8. The composition of claim 7 , wherein the additive is MgO or ZnO. 9. The composition of claim 7 , wherein the first composition is present in an amount from 26 wt % to 42 wt %, based on the weight of the composition. 10. The composition of claim 7 , wherein the composition, after 1008 hours, at 150° C., in air, retains ≥50% of its original Tensile Strength, and retains ≥35% of its original Elongation at Break. 11. A crosslinked composition comprising the composition of claim 7 . 12. An article comprising at least one component formed from the composition of claim 7 . 13. The composition of claim 1 , wherein the composition, after 1008 hours, at 150° C., in air, retains ≥50% of its original Tensile Strength, and retains ≥35% of its original Elongation at Break.
Ethylene-propylene or ethylene-propylene-diene copolymers · CPC title
with non-conjugated dienes, e.g. EPT rubbers · CPC title
containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure · CPC title
Crosslinking · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.