Method for recovering valuable metal
US-11807914-B2 · Nov 7, 2023 · US
US11959151B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11959151-B2 |
| Application number | US-201816641669-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 21, 2018 |
| Priority date | Sep 29, 2017 |
| Publication date | Apr 16, 2024 |
| Grant date | Apr 16, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a method for separating copper from nickel and cobalt, which is capable of efficiently and selectively separating copper, and nickel and cobalt from an alloy containing copper, nickel and cobalt such as a highly anticorrosive alloy that is obtained by subjecting a waste lithium ion battery to a dry treatment and contains copper, nickel and cobalt. According to the present invention, an alloy containing copper, nickel and cobalt is brought into contact with an acid in the coexistence of a sulfurization agent, thereby obtaining a solid that contains copper and a leachate that contains nickel and cobalt.
Opening claim text (preview).
The invention claimed is: 1. A separation method for separating copper, nickel and cobalt from an alloy obtained by melting and reducing a waste lithium ion battery, the method comprising producing the alloy in the form of an alloy powder, the alloy powder containing a copper metal, a nickel metal, and a cobalt metal; adding a sulfurization agent to the alloy powder to establish a state of the sulfurization agent and the alloy powder coexisting; wherein the sulfurization agent is one or more selected from the group consisting of elemental sulfur, hydrogen sulfide gas, sodium hydrogen sulfide and sodium sulfide; and bringing the sulfurization agent and the alloy powder coexisting into contact with hydrochloric acid whereby the nickel metal and the cobalt metal are leached from the alloy powder and the copper metal contained in the alloy powder is sulfurized by the sulfurization agent to obtain a solid containing copper sulfide and a leachate containing the nickel existing as an ion and the cobalt existing as an ion. 2. The separation method according to claim 1 , wherein the alloy powder has a particle size of 300 μm or less. 3. The separation method according to claim 1 , wherein the solid containing the copper sulfide and the leachate containing the nickel and the cobalt are separated, and then copper remaining in the leachate is removed. 4. The separation method according to claim 3 , wherein a copper remaining in the leachate is removed by one or more methods selected from sulfurization, electrolytic winning and neutralization precipitation.
Reduction smelting or converting · CPC title
Hydrochloric acid {, other halogenated acids or salts thereof} · CPC title
Scrap treating · CPC title
by gases, e.g. hydrogen or hydrogen sulfide · CPC title
Sulfuric acid {, other sulfurated acids or salts thereof} · CPC title
Related publications grouped by family.