Positive electrode active material and preparation method thereof, secondary battery, battery module, battery pack and electrical device
US-2024387819-A1 · Nov 21, 2024 · US
US11909039B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11909039-B2 |
| Application number | US-202016749208-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 22, 2020 |
| Priority date | Oct 30, 2014 |
| Publication date | Feb 20, 2024 |
| Grant date | Feb 20, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The nickel-containing composite hydroxide disclosed herein contain secondary particles, which are formed from an aggregation of numerous primary particles, which have an average particle size of the primary particles is 0.01 μm to 0.40 μm. These secondary particles have a spherical or ellipsoidal shape, an average particle size of 20 μm to 50 μm, and a BET value of 12 m2/g to 50 m2/g after being roasted in air for 2 hours at 800° C.
Opening claim text (preview).
What is claimed is: 1. A nickel-containing composite hydroxide that is expressed by the general formula: Ni 1-x-y Co x Al y M t (OH) 2+α , where, 0≤x≤0.20, 0≤y≤0.15, 0≤t≤0.10, 0≤α≤0.50, and M is one or more kind of element selected from among Mg, Ca, Ba, Nb, Mo, V, Ti, Zr and Y, or the general formula: Ni 1-x-z Co x Mn z M t (OH) 2+α , where 0≤x≤0.50, 0≤z≤0.50, x+z≤0.70, 0≤t≤0.10, 0≤α≤0.50, and M is one or more kind of element selected from among Mg, Ca, Ba, Nb, Mo, V, Ti, Zr and Y, the nickel-containing composite hydroxide comprising secondary particles, each of the secondary particles being formed from an aggregation of a plurality of primary particles, wherein the shape of each of the secondary particles is spherical or ellipsoidal, wherein the average particle size of the secondary particles is 20 μm to 50 μm, and the average particle size of the primary particles is 0.01 μm to 0.40 μm, and the BET value after roasting the nickel-containing composite hydroxide in air for 2 hours at 800° C. is 12 m 2 /g to 50 m 2 /g. 2. The nickel-containing composite hydroxide according to claim 1 , wherein the average particle size of the secondary particles is 25 μm to 50 μm.
Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements · CPC title
of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy · CPC title
Chemistry & Metallurgy · mapped topic
containing alkali metals, e.g. LiNiO2 · CPC title
of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2 · CPC title