Electrode for non-aqueous electrolyte secondary battery
US-2020365881-A1 · Nov 19, 2020 · US
US11876229B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11876229-B2 |
| Application number | US-202017274590-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 28, 2020 |
| Priority date | Jan 28, 2019 |
| Publication date | Jan 16, 2024 |
| Grant date | Jan 16, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed is a negative electrode including: a current collector; a negative electrode active material layer disposed on at least one surface of the current collector, including a silicon-based active material and a conductive material, and containing no binder polymer; and a coating layer disposed on the surface of the negative electrode active material layer and in at least a part of the inside of the pores of the negative electrode active material layer, and containing a coating layer polymer forming a chemical bond with silicon (Si) of the silicon-based active material, wherein the content of the coating layer polymer is 0.3-2 parts by weight based on 100 parts by weight of the negative electrode active material layer, and the coating layer polymer is a mixture of polyacrylic acid with polyvinyl alcohol.
Opening claim text (preview).
What is claimed is: 1. A negative electrode comprising: a current collector; a negative electrode active material layer disposed on at least one surface of the current collector, comprising a silicon-based active material and a conductive material, and containing no binder polymer; and a coating layer disposed on a surface of the negative electrode active material layer and at least a part of inside of pores of the negative electrode active material layer, and containing a coating layer polymer forming a chemical bond with silicon (Si) of the silicon-based active material, wherein a content of the coating layer polymer is 0.3-2 parts by weight based on 100 parts by weight of the negative electrode active material layer, and the coating layer polymer comprises a mixture of polyacrylic acid with polyvinyl alcohol. 2. The negative electrode according to claim 1 , wherein the content of the coating layer polymer is 0.5-1.5 parts by weight based on 100 parts by weight of the negative electrode active material layer. 3. The negative electrode according to claim 1 , wherein the coating layer polymer comprises polyacrylic acid and polyvinyl alcohol at a weight ratio of 9:1-1:9. 4. The negative electrode according to claim 1 , wherein the negative electrode active material layer consists essentially of the silicon-based active material and the conductive material. 5. A method for manufacturing a negative electrode, comprising: forming a negative electrode active material layer comprising a silicon-based active material and a conductive material and containing no binder polymer onto at least one surface of a current collector; coating a composition for a coating layer comprising a coating layer polymer and a solvent on a surface of the negative electrode active material layer and at least a part of inside of pores of the negative electrode active material layer; and drying the coated composition for a coating layer at 140-190° C. to form a coating layer in which the coating layer polymer forms a chemical bond with silicon (Si) of the silicon-based active material, wherein a content of the coating layer polymer is 0.3-2 parts by weight based on 100 parts by weight of the negative electrode active material layer, and the coating layer polymer comprises a mixture of polyacrylic acid with polyvinyl alcohol. 6. The method for manufacturing a negative electrode according to claim 5 , wherein the content of the coating layer polymer is 0.5-1.5 parts by weight based on 100 parts by weight of the negative electrode active material layer. 7. The method for manufacturing a negative electrode according to claim 5 , wherein the negative electrode active material layer consists essentially of the silicon-based active material and the conductive material. 8. The method for manufacturing a negative electrode according to claim 5 , wherein the coating is carried out through dip coating, spray coating, die coating or a combination of at least two thereof. 9. A lithium secondary battery comprising the negative electrode according to claim 1 .
Selection of inactive substances as ingredients for active masses, e.g. binders, fillers · CPC title
by coating on electrode collectors · CPC title
involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis · CPC title
Electrodes based on metals, Si or alloys · CPC title