Stable biodegradable receptacle
US-2024270467-A1 · Aug 15, 2024 · US
US11873607B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11873607-B2 |
| Application number | US-201916543224-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 16, 2019 |
| Priority date | Nov 17, 2014 |
| Publication date | Jan 16, 2024 |
| Grant date | Jan 16, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided herein is a tobacco packaging material, comprising a paper material coated with at least one polymer layer. The polymer layer comprises at least one repulpable polymer, and wherein the tobacco packaging material has a water vapor transmission rate (WVTR) that is at least 90% lower than the paper material. Further provided is a tobacco package comprising the tobacco packaging material, wherein the tobacco package is substantially free of any foil inner liner or polypropylene film. Further described is a method for making the tobacco packaging material, comprising extrusion coating at least one repulpable polymer onto a paper material to form a polymer layer, and optionally further depositing at least one atomic layer deposition (ALD) layer that comprises a metal oxide.
Opening claim text (preview).
That which is claimed: 1. A method for making a tobacco packaging material, the method comprising: extrusion coating at least one repulpable polymer onto a paper material to form a polymer layer; depositing at least two atomic layer deposition (ALD) layers onto the paper material coated with the polymer layer, wherein the at least two ALD layers comprises at least one metal oxide layer and at least one elastic metal oxide/organic layer; and heat treating the paper material coated with the polymer layer prior to depositing the at least two ALD layers, wherein the tobacco packaging material has a water vapor transmission rate (WVTR) that is at least 90% lower than the paper material. 2. The method of claim 1 , wherein the polymer layer comprises a polymer selected from the group consisting of polyglycolic acid (PGA) and polylactic acid (PLA). 3. The method of claim 1 , wherein the paper material is coated with at least two polymer layers having different crystallinity. 4. The method of claim 1 , wherein the paper material is coated with about 1-200 g/m 2 of the polymer. 5. The method of claim 1 , wherein the at least two ALD layers comprise a metal oxide selected from the group consisting of Al 2 O 3 and SiO 2 . 6. The method of claim 1 , wherein the tobacco packaging material has a WVTR of 10 g/m 2 /day or less at 38° C. and 90% RH. 7. The method of claim 1 , wherein the tobacco packaging material has a WVTR of 3.4 g/m 2 /day or less at 38° C. and 90% RH.
Sizing or water-repelling agents · CPC title
applied in non-semiconductor technology · CPC title
superposed {(D21H19/84 takes precedence)} · CPC title
Packing paper (packaging materials of special type or form B65D65/38) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.