Solid binders
US-2019382583-A1 · Dec 19, 2019 · US
US11873406B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11873406-B2 |
| Application number | US-201917296410-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 6, 2019 |
| Priority date | Dec 10, 2018 |
| Publication date | Jan 16, 2024 |
| Grant date | Jan 16, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A bituminous composition comprising at least one bitumen base, at least one compound of general formula (I): Ar1-R 1 —Ar 2 (I), and at least one compound of general formula (II): R 2 —(NH) n CONH—X—(NHCO) p (NH) n —R′ 2 (II). The invention also concerns a process for the preparation of said bituminous composition.
Opening claim text (preview).
The invention claimed is: 1. A bituminous composition comprising at least: a) a bitumen base, b) 2′,3-bis[(3-[3,5-di(tert-butyl)-4-hydroxyphenyl]propionyl)]propionohydrazide, and c) N,N′-ethylenedi(stearamide) of formula C 17 H 35 —CONH—CH 2 —CH 2 —NHCO—C 17 H 35 . 2. The bituminous composition as claimed in claim 1 , comprising from 0.1 to 10% by weight of 2′,3-bis[(3-[3,5-di(tert-butyl)-4-hydroxyphenyl]propionyl)]propionohydrazide with respect to the total weight of the bituminous composition. 3. The bituminous composition as claimed in claim 1 , comprising from 0.1% to 10% by weight of N,N′-ethylenedi(stearamide) of formula C 17 H 35 —CONH—CH 2 —CH 2 —NHCO—C 17 H 35 by weight, with respect to the total weight of the bituminous composition. 4. The bituminous composition as claimed in claim 1 , comprising from 80 to 99.8% by weight of one or several bitumen bases, with respect to the total weight of the bituminous composition. 5. The bituminous composition as claimed in claim 1 , comprising: a) from 80 to 99.8% by weight of one or several bitumen bases, b) from 0.1 to 10% by weight of 2′,3-bis[(3-[3,5-di(tert-butyl)-4-hydroxyphenyl]propionyl)]propionohydrazide, and c) from 0.1 to 10% by weight of N,N′-ethylenedi(stearamide) of formula C 17 H 35 —CONH—CH 2 —CH 2 —NHCO—C 17 H 35 , with respect to the total weight of the bituminous composition. 6. The bituminous composition as claimed in claim 1 , wherein the bitumen base has a penetrability at 25° C., measured according to standard EN 1426, lower than or equal to 200 1/10 mm. 7. The bituminous composition as claimed in claim 1 , having a penetrability at 25° C., measured according to standard EN 1426, lower than or equal to 40 1/10 mm. 8. The bituminous composition as claimed in claim 1 , having a ring-and-ball softening point, measured according to standard EN 1427, of from 80 to 120° C. 9. The bituminous composition as claimed in claim 1 , having a deformability at 65° C. lower than or equal to 50%. 10. The bituminous composition as claimed in claim 1 , having a viscosity at 160° C., V160, measured according to standard EN 13702, lower than or equal to 500 mPa·s. 11. A process for the preparation of a bituminous composition according to claim 1 , said process comprising contacting, at a temperature ranging from 70° C. to 220° C., the bitumen base with 2′,3-bis[(3-[3,5-di(tert-butyl)-4-hydroxyphenyl]propionyl)]propionohydrazide and N,N′-ethylenedi(stearamide) of formula C 17 H 35 —CONH—CH 2 —CH 2 —NHCO—C 17 H 35 . 12. The process according to claim 11 , which comprises the following steps: a) the introduction of the bitumen base in a reactor equipped with mixing means and its heating at a temperature ranging from 70° C. to 220° C., b) the simultaneous or successive additions of 2′,3-bis[(3-[3,5-di(tert-butyl)-4-hydroxyphenyl]propionyl)]propionohydrazide and N,N′-ethylenedi(stearamide) of formula C 17 H 35 —CONH—CH 2 —CH 2 —NHCO—C 17 H 35 , and c) the mixture of the bituminous composition at a temperature ranging from 70° C. to 220° C., until obtaining a homogenous composition.