Method for producing sintered ferrite magnet, and sintered ferrite magnet
US-9162928-B2 · Oct 20, 2015 · US
US11810699B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11810699-B2 |
| Application number | US-201716469833-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 22, 2017 |
| Priority date | Dec 22, 2016 |
| Publication date | Nov 7, 2023 |
| Grant date | Nov 7, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a ferrite sintered magnet including a ferrite phase having a magnetoplumbite-type crystal structure. x, y, and m satisfy the following Equations (1), (2), and (3) when composition of the ferrite sintered magnet is represented by R 1-x A x Fe m-y Co y , where R denotes at least one kind of element selected from rare earth elements including Y and A denotes Ca or Ca and elements including at least one kind selected from Sr or Ba. The content of B in the ferrite sintered magnet is from 0.1% to 0.6% by mass in terms of B 2 O 3 . 0.2≤ x ≤0.8 (1) 0.1≤ y ≤0.65 (2) 3≤ m <14 (3)
Opening claim text (preview).
The invention claimed is: 1. A ferrite sintered magnet comprising a ferrite phase having a magnetoplumbite-type crystal structure, wherein x1, x2, y, and m satisfy the following Equations (6), (7), (8) and (9) when composition of the ferrite sintered magnet is represented by R 1-x1-x2 Ca x1 Sr x2 Fe m-y Co y , where R denotes at least one kind of element selected from rare earth elements including Y: 0.2≤ x 1≤0.5 (6) 0≤ x 2≤0.1 (7) 0.2≤ y ≤0.4 (8) 6.5≤ m ≤9.5 (9), a content of B is from 0.2% to 0.4% by mass or less in terms of B 2 O 3 , and a content of Si is less than 0.3% by mass when Si is converted into SiO 2 , and wherein a coercive force of the ferrite sintered magnet at 20° C. is 652 Oe or more. 2. The ferrite sintered magnet according to claim 1 , wherein the following Equations (4) and (5) are satisfied: 0.2≤ x 1 +x 2<0.55 (4) 7.5< m≤ 9.5 (5). 3. A motor comprising the ferrite sintered magnet according to claim 1 . 4. A generator comprising the ferrite sintered magnet according to claim 1 .
in the form of particles {(for magnetic record carriers G11B5/70626)} · CPC title
containing barium, strontium or calcium · CPC title
of calcined, sintered clinker or ceramics · CPC title
Wet mixtures · CPC title
Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F}) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.