Tearable tube formed from fluororesin
US-2018281262-A1 · Oct 4, 2018 · US
US11802199B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11802199-B2 |
| Application number | US-201816959976-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 5, 2018 |
| Priority date | Jan 4, 2018 |
| Publication date | Oct 31, 2023 |
| Grant date | Oct 31, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
There is provided a thermoplastic fluororesin tube that, during the production of a catheter, can prevent a gap or air bubbles from being formed in the connection part of the catheter, and can be suitably used for the production of a catheter. A thermoplastic fluororesin tube, the thermoplastic fluororesin tube having tearability in a longitudinal direction, wherein a thermal expansion coefficient in the longitudinal direction upon heating in a gaseous phase at a temperature of 100° C. for 5 minutes is 0% or more.
Opening claim text (preview).
The invention claimed is: 1. A method for producing a thermoplastic fluororesin tube comprising a tetrafluoroethylene-hexafluoropropylene-perfluoroalkyl vinyl ether copolymer (FEP), the thermoplastic fluororesin tube having tearability in a longitudinal direction, wherein a thermal expansion coefficient in the longitudinal direction upon heating in a gaseous phase at a temperature of 100° C. for 5 minutes is 0% or more, the method comprising the steps of: subjecting a thermoplastic fluororesin comprising a tetrafluoroethylene-hexafluoropropylene-perfluoroalkyl vinyl ether copolymer (FEP) to melt extrusion molding to obtain a raw tube of the thermoplastic fluororesin tube; and expanding an inner diameter of the raw tube while heating the raw tube to a temperature of from 110-135° C. 2. The method according to claim 1 , wherein the thermoplastic fluororesin further comprises a tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA). 3. The method according to claim 1 , wherein a heat shrinkage ratio of an inner diameter of the thermoplastic fluororesin tube, upon heating in a gaseous phase at a temperature of 200° C. for 5 minutes, is 51% or more. 4. The method according to claim 1 , wherein the thermal expansion coefficient in the longitudinal direction upon heating at a temperature of 100° C. for 5 minutes is 0 to 4%. 5. The method according to claim 1 , which comprises a weld line in the longitudinal direction. 6. The method according to claim 1 , wherein a tear strength of the thermoplastic fluororesin tube is 12 N/mm or less.
by stretching tubes {(in general B29C55/22, B29C55/28)} · CPC title
Homopolymers or copolymers of hexafluoropropene · CPC title
combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence) · CPC title
Homopolymers or copolymers or tetrafluoroethene · CPC title
Making of catheters or other medical or surgical tubes · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.