Catalyst composition, a process for preparing the catalyst composition and a use of the catalyst composition
US-8932979-B2 · Jan 13, 2015 · US
US11801493B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11801493-B2 |
| Application number | US-201716465445-A |
| Country | US |
| Kind code | B2 |
| Filing date | Nov 29, 2017 |
| Priority date | Dec 2, 2016 |
| Publication date | Oct 31, 2023 |
| Grant date | Oct 31, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Methods for conditioning an ethylene epoxidation catalyst are provided. The conditioning methods comprise contacting an ethylene epoxidation catalyst comprising a carrier, having silver and a rhenium promoter deposited thereon, with a conditioning feed gas comprising oxygen for a period of time of at least 2 hours at a temperature that is above 180° C. and at most 250° C., wherein the contacting of the ethylene epoxidation catalyst with the conditioning feed gas occurs in an epoxidation reactor and in the absence of ethylene. Associated methods for the epoxidation of ethylene are also provided.
Opening claim text (preview).
That which is claimed is: 1. A method for the conditioning of an ethylene epoxidation catalyst comprising: contacting an ethylene epoxidation catalyst comprising a carrier, having silver and a rhenium promoter deposited thereon, with a conditioning feed gas consisting essentially of oxygen, an inert gas and, optionally, an organic chloride, for a period of time of from 6 to 72 hours at a temperature that is, from at least 185° C. and at most 220° C., wherein the contacting of the ethylene epoxidation catalyst with the conditioning feed gas occurs in a catalyst bed within an epoxidation reactor and in the absence of ethylene, and wherein the catalyst bed comprises the ethylene epoxidation catalyst. 2. The method of claim 1 wherein the conditioning feed gas comprises oxygen in a concentration of from 0.5 to 21 mole %, relative to the total conditioning feed gas. 3. The method of claim 1 wherein the period of time is from 12 to 72 hours. 4. The method of claim 1 wherein the period of time is from 24 hours to 72 hours. 5. The method of claim 1 further comprising contacting the ethylene epoxidation catalyst with a sweeping gas. 6. The method of claim 1 , wherein the inert gas is selected from nitrogen, methane, argon, helium, and a combination thereof.
with manganese, technetium or rhenium · CPC title
Heat treatment {(B01J37/0009, B01J37/0018 take precedence)} · CPC title
with gases containing free oxygen · CPC title
with catalysts containing silver or gold · CPC title
containing only hydrogen and carbon atoms in addition to the ring oxygen atoms · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.