Slow-release inhibitor for high-magnesium sulfide mineral flotation and application thereof

US11779935B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-11779935-B2
Application numberUS-201916693186-A
CountryUS
Kind codeB2
Filing dateNov 22, 2019
Priority dateApr 10, 2019
Publication dateOct 10, 2023
Grant dateOct 10, 2023

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed are a slow-release inhibitor for high-magnesium sulfide mineral flotation and an application thereof, where the inhibitor is a nano colloidal particle of an alkaline earth fluoride such as CaF2 and BaF2 or a highly-reactive natural alkaline earth metal mineral powder. When applied to the flotation separation of a high-magnesium sulfide ore, the inhibitor can slowly release F ions to preferentially form a MgF2 layer on the magnesium-containing mineral surface, which provides a structure similar to MgF2 on a surface of oxidized gangue minerals such as magnesium oxide, changing surface electrical property of the magnesium-containing mineral, inhibiting heterogeneous coagulation of magnesium-containing minerals and sulfide ores due to electrostatic attraction and reducing entrainment, enveloping and agglomeration of gangue minerals to efficiently inhibit the flotation of oxidized gangue minerals such as magnesium oxide.

First claim

Opening claim text (preview).

What is claimed is: 1. A method of separating a high-magnesium sulfide ore, comprising: mixing alkaline earth metal fluoride in the form of a nano alkaline earth fluoride colloidal particle or in the form of a natural alkaline earth metal mineral with the high-magnesium sulfide mineral to produce an ore pulp; stirring the ore pulp under 1,200-3,000 rpm for 5-30 min; and introducing a collector to obtain a flotation system. 2. The method of claim 1 , wherein a mass ratio of the nano alkaline earth fluoride colloidal particle or the natural alkaline earth metal mineral to the high-magnesium sulfide mineral is 1:10-500; and a pulping time is 5-30 min. 3. The method of claim 1 , wherein a concentration of the ore pulp in the flotation is controlled at 30%-40%, and a pH of the flotation system is controlled to 7-9. 4. The method of claim 1 , wherein the nano alkaline earth fluoride colloidal particle or the natural alkaline earth metal mineral is used in combination with at least one of acidified sodium silicate, sodium hexametaphosphate, starch and tannin. 5. The method of claim 1 , wherein the collector is selected from the group consisting of copper sulfide, cobalt sulfide and nickel sulfide. 6. A method of separating a high-magnesium sulfide ore, comprising: mixing alkaline earth metal fluoride in the form of a nano alkaline earth fluoride colloidal particle or in the form of a natural alkaline earth metal mineral with the high-magnesium sulfide mineral to produce an ore pulp; stirring the ore pulp under 1,200-3,000 rpm for 5-30 min; and introducing a collector to obtain a flotation system; wherein the high-magnesium sulfide ore comprises at least one magnesium-containing gangue mineral selected from magnesite, serpentine, talc, olivine, pyroxene, hornblende, biotite, chlorite, vermiculite, montmorillonite and illite, and at least one metal sulfide ore selected from nickel sulfide mineral, cobalt sulfide mineral and copper sulfide mineral. 7. The method of claim 5 , wherein a mass ratio of the nano alkaline earth fluoride colloidal particle or the natural alkaline earth metal mineral to the high-magnesium sulfide mineral is 1:10-500; and a pulping time is 5-30 min. 8. The method of claim 5 , wherein the nano alkaline earth fluoride colloidal particle or the natural alkaline earth metal mineral is used in combination with at least one of acidified sodium silicate, sodium hexametaphosphate, starch and tannin. 9. The method of claim 6 , wherein the collector is selected from the group consisting of copper sulfide, cobalt sulfide and nickel sulfide.

Assignees

Inventors

Classifications

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US11779935B2 cover?
Disclosed are a slow-release inhibitor for high-magnesium sulfide mineral flotation and an application thereof, where the inhibitor is a nano colloidal particle of an alkaline earth fluoride such as CaF2 and BaF2 or a highly-reactive natural alkaline earth metal mineral powder. When applied to the flotation separation of a high-magnesium sulfide ore, the inhibitor can slowly release F ions to p…
Who is the assignee on this patent?
Univ Central South
What technology area does this patent fall under?
Primary CPC classification B03D1/002. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Oct 10 2023 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).