Functionalized nitrile rubbers and the production thereof
US-10011664-B2 · Jul 3, 2018 · US
US11713362B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11713362-B2 |
| Application number | US-202017135344-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 28, 2020 |
| Priority date | Dec 28, 2020 |
| Publication date | Aug 1, 2023 |
| Grant date | Aug 1, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A depolymerizer is formed by grafting thiol groups on parts of the double bonds of a polymer of linear conjugated diene monomer. The linear conjugated diene monomer can be 1,3-butadiene, isoprene, 1,3-pentadiene, 2,3-dimethyl-1,3-butadiene, 2-methyl-1,3-pentadiene, 2,3-dimethyl-1,3-pentadiene, 2-phenyl-1,3-butadiene, or 4,5-diethyl-1,3-octadiene. The depolymerizer has a weight average molecular weight of 1000 to 400000.
Opening claim text (preview).
What is claimed is: 1. A depolymerizer, having a chemical structure of wherein (a+a′+b+b′):(m+n)=0.01:1 to 0.67:1, a>0, a′>0, b>0, and b′>0. 2. The depolymerizer as claimed in claim 1 , having a weight average molecular weight of 1000 to 400000. 3. A recycled rubber, being formed by depolymerizing 100 parts by weight of rubber using 0.5 to 10 parts by weight of a depolymerizer, wherein the depolymerizer has a chemical structure of wherein (a+a′+b+b′):(m+n)=0.01:1 to 0.67:1, a′>0 b>0, and b′>0. 4. The recycled rubber as claimed in claim 3 , wherein the rubber comprises poly(cis-1,3-butadiene) rubber, polystyrene-butadiene rubber, nitrile rubber, buna rubber, ethylene propylene rubber, butyl rubber, or a combination thereof. 5. The recycled rubber as claimed in claim 3 , wherein the depolymerizer has a weight average molecular weight of 1000 to 400000.
Devulcanisation · CPC title
Depolymerisation · CPC title
Addition of a reagent which reacts with a hetero atom or a group containing hetero atoms of the macromolecule · CPC title
containing elements other than carbon and hydrogen · CPC title
Incorporating sulfur atoms into the molecule · CPC title