Stabilized fiber, method of producing the same, and method of producing carbon fiber

US11702769B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-11702769-B2
Application numberUS-202017019526-A
CountryUS
Kind codeB2
Filing dateSep 14, 2020
Priority dateSep 19, 2019
Publication dateJul 18, 2023
Grant dateJul 18, 2023

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A method of producing a stabilized fiber, including performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex.

First claim

Opening claim text (preview).

What is claimed is: 1. A method of producing a stabilized fiber, comprising performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex, wherein the heat treatment is performed until an intensity ratio of a G peak near 1,590 cm −1 to a D peak near 1,360 cm −1 in a Raman spectrum on a side of the acrylamide polymer fiber becomes 0.5 or more, wherein an acrylamide polymer used in the acrylamide polymer fiber is a homopolymer of an acrylamide monomer or a copolymer of an acrylamide monomer and other polymerizable monomers in which a content of the acrylamide monomer unit in the copolymer is 50 mol % or more. 2. A method of producing a carbon fiber, comprising: producing the stabilized fiber using the method according to claim 1 ; and performing carbonization on the stabilized fiber. 3. A method of producing a stabilized fiber, comprising, performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex wherein the heat treatment is performed until a density of the acrylamide polymer fiber becomes 1.35 g/cm 3 to 1.75 g/cm 3 , wherein an acrylamide polymer used in the acrylamide polymer fiber is a homopolymer of an acrylamide monomer or a copolymer of an acrylamide monomer and other polymerizable monomers in which a content of the acrylamide monomer unit in the copolymer is 50 mol % or more. 4. A method of producing a carbon fiber, comprising: producing the stabilized fiber using the method according to claim 3 ; and performing carbonization on the stabilized fiber. 5. A stabilized fiber which is derived from an acrylamide polymer and has an intensity ratio of 0.5 or more of a G peak near 1,590 cm −1 to a D peak near 1,360 cm −1 in a Raman spectrum on the side of the fiber, wherein the acrylamide polymer is a homopolymer of an acrylamide monomer or a copolymer of an acrylamide monomer and other polymerizable monomers in which a content of the acrylamide monomer unit in the copolymer is 50 mol % or more. 6. A method of producing a carbon fiber, comprising performing carbonization on the stabilized fiber according to claim 5 . 7. A stabilized fiber which is derived from an acrylamide polymer and has a density of 1.35 g/cm 3 to 1.75 g/cm 3 , wherein the acrylamide polymer is a homopolymer of an acrylamide monomer or a copolymer of an acrylamide monomer and other polymerizable monomers in which a content of the acrylamide monomer unit in the copolymer is 50 mol % or more. 8. A method of producing a carbon fiber, comprising performing carbonization on the stabilized fiber according to claim 7 .

Assignees

Inventors

Classifications

  • D01F9/225Primary

    from stabilised polyacrylonitriles · CPC title

  • Carbon (carbon nanotubes C04B14/026) · CPC title

  • Carbon; Pitch · CPC title

  • D01F9/21Primary

    from macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds · CPC title

  • D01D10/02Primary

    Heat treatment (heating for finishing D02J13/00) · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US11702769B2 cover?
A method of producing a stabilized fiber, including performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex.
Who is the assignee on this patent?
Toyota Motor Co Ltd, Toyota Chuo Kenkyusho Kk
What technology area does this patent fall under?
Primary CPC classification D01F9/225. Mapped technology areas include Textiles & Paper.
When was this patent published?
Publication date Tue Jul 18 2023 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).