Stationary semi-solid battery module and method of manufacture
US-9203092-B2 · Dec 1, 2015 · US
US11652203B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11652203-B2 |
| Application number | US-202117410696-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 24, 2021 |
| Priority date | Jul 9, 2018 |
| Publication date | May 16, 2023 |
| Grant date | May 16, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Embodiments described herein relate generally to systems and methods for continuously and/or semi-continuously manufacturing semi-solid electrodes and batteries incorporating semi-solid electrodes. In some embodiments, the process of manufacturing a semi-solid electrode includes continuously dispensing a semi-solid electrode slurry onto a current collector, separating the semi-solid electrode slurry into discrete portions, and cutting the current collector to form a finished electrode.
Opening claim text (preview).
The invention claimed is: 1. A method, comprising: disposing a current collector material on a first plate and a second plate; moving the first plate relative to the second plate, such that a first portion of the current collector material is on the first plate, a second portion of the current collector material is on the second plate, and a third portion of the current collector material is clamped between the first plate and the second plate; continuously dispensing a semi-solid electrode material onto the first portion of the current collector material and the second portion of the current collector material; and moving the second plate relative to the first plate, such that the first portion of the current collector material moves relative to the second portion of the current collector material, and the third portion of the current collector material is released from between the first plate and the second plate, the third portion of the current collector being uncoated. 2. The method of claim 1 , wherein the semi-solid electrode material is binderless. 3. The method of claim 1 , further comprising: pushing and/or pulling the third portion of the current collector material between the first portion of the current collector material and the second portion of the current collector material via a tucking device. 4. The method of claim 1 , wherein the first plate and the second plate are movable between a first configuration and a second configuration, an edge of the first plate abutting an edge of the second plate to frictionally engage the third portion of the current collector material in the first configuration, the edge of the first plate separated from the edge of the second plate in the second configuration so that the portion of the third current collector material can be removed from between the two plates. 5. The method of claim 1 , further comprising: adjoining a portion of the semi-solid electrode material with a second electrode interposed by a separator to form a finished electrochemical cell. 6. The method of claim 1 , further comprising: inspecting the semi-solid electrode material via a video camera and computer processor. 7. The method of claim 1 , wherein moving the second plate relative to the first plate is via rotating the first plate away from the second plate. 8. The method of claim 1 , further comprising: conveying the first plate and the second plate via a conveyor. 9. The method of claim 8 , wherein the conveyor includes a vacuum pallet. 10. A method, comprising: disposing a current collector material on a first pallet and a second pallet; moving the first pallet relative to the second pallet, such that a first portion of the current collector material is on the first pallet, a second portion of the current collector material is on the second pallet, and a third portion of the current collector material is clamped between the first pallet and the second pallet; dispensing a semi-solid electrode material onto the first portion of the current collector material and the second portion of the current collector material; and moving the second pallet relative to the first pallet, such that the first portion of the current collector material moves relative to the second portion of the current collector material, and the third portion of the current collector material is released from between the first pallet and the second pallet, the third portion of the current collector being uncoated. 11. The method of claim 10 , wherein the semi-solid electrode slurry is binderless. 12. The method of claim 10 , further comprising: pushing and/or pulling the third portion of the current collector material between the first portion of the current collector material and the second portion of the current collector material via a tucking device. 13. The method of claim 10 , wherein the first pallet has a first securing edge and the second pallet has a second securing edge, the first securing edge abutting the second securing edge to frictionally engage the third portion of the current collector material. 14. The method of claim 10 , further comprising: adjoining a portion of the semi-solid electrode material with a second electrode interposed by a separator to form a finished electrochemical cell. 15. The method of claim 10 , wherein moving the second pallet relative to the first pallet is via rotating the first pallet away from the second pallet. 16. The method of claim 10 , further comprising: conveying the first pallet and the second pallet via a conveyor. 17. The method of claim 16 , wherein the conveyor includes a vacuum pallet. 18. A method, comprising: placing a current collector material on a first plate and a second plate; moving the first plate relative to the second plate, such that a first portion of the current collector material is on the first plate, a second portion of the current collector material is on the second plate, and a third portion of the current collector material is clamped between the first plate and the second plate; dispensing a semi-solid electrode material onto the first portion of the current collector material and the second portion of the current collector material; and rotating the second plate relative to the first plate, such that the first portion of the current collector material moves relative to the second portion of the current collector material, and the third portion of the current collector material is released from between the first plate and the second plate, the third portion of the current collector being uncoated. 19. The method of claim 18 , wherein the semi-solid electrode slurry is binderless. 20. The method of claim 18 , further comprising: pushing and/or pulling the third portion of the current collector material between the first portion of the current collector material and the second portion of the current collector material via a tucking device. 21. The method of claim 18 , wherein the first plate has a first securing edge and the second plate has a second securing edge, the first securing edge abutting the second securing edge to frictionally engage the third portion of the current collector material. 22. The method of claim 18 , further comprising: adjoining a portion of the semi-solid electrode material with a second electrode interposed by a separator to form a finished electrochemical cell. 23. The method of claim 18 , further comprising: conveying the first plate and the second plate via a conveyor. 24. The method of claim 23 , wherein the conveyor includes a vacuum pallet.
Energy storage using batteries · CPC title
Li-accumulators · CPC title
Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium · CPC title
Construction or manufacture · CPC title
Construction or manufacture in general (H01M10/058, H01M10/12, H01M10/28, H01M10/38 take precedence) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.