Method of producing grain-oriented electrical steel sheet
US-2024249863-A1 · Jul 25, 2024 · US
US11615902B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11615902-B2 |
| Application number | US-202016798870-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 24, 2020 |
| Priority date | Feb 28, 2019 |
| Publication date | Mar 28, 2023 |
| Grant date | Mar 28, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A soft magnetic alloy powder contains Fe, Si, and at least one of Cr and Al, as constituent elements, wherein, on the surface of each grain constituting the alloy powder, an oxide film is provided which is such that: it contains Si, as well as at least one of Cr and Al, as constituent elements; these elements are contained at higher percentages by mass than those in the alloy part inside the grain; and the content of Si, expressed in percentage by mass, is higher than the total content of Cr and Al. The soft magnetic metal powder can achieve a higher filling rate.
Opening claim text (preview).
We claim: 1. A soft magnetic alloy powder containing Fe, Si, and at least one of Cr and Al, as constituent elements, wherein, on a surface of each grain constituting the alloy powder, an oxide film is formed, wherein: the oxide film contains Si, as well as at least one of Cr and Al, as constituent elements; the Si and the at least one of Cr and Al are contained at higher percentages by mass than those in an alloy part of the grain underneath the oxide film; and a content of the Si, expressed in percentage by mass, is higher than a total content of the at least one of Cr and Al. 2. The soft magnetic alloy powder according to claim 1 , whose specific surface area S (m 2 /g) and average grain size D 50 (μm) satisfy Formula (1) below: log S≤− 0.98 log D 50 +0.34 (1). 3. The soft magnetic alloy powder according to claim 1 , wherein a Si/Cr ratio by mass or Si/Al ratio by mass at a topmost surface of the oxide film is in a range from 1 to 10. 4. The soft magnetic alloy powder according to claim 1 , wherein a composition of the alloy part is such that Si is contained by 1 to 10 percent by mass, Cr or Al is contained by 0.2 to 2 percent by mass in total, and a remainder is Fe and unavoidable impurities. 5. The soft magnetic alloy powder according to claim 1 , wherein: Fe, Si, and Al are contained as constituent elements; and a composition of the alloy part is such that Si is contained by 1 to 10 percent by mass, Al is contained by 0.2 to 1 percent by mass, and a remainder is Fe and unavoidable impurities. 6. The soft magnetic alloy powder according to claim 1 , wherein Fe is detected at any given locations of the oxide film.
Thermal or thermo-mechanical treatment · CPC title
Fe-Si-Al based alloys, e.g. Sendust · CPC title
Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10) · CPC title
Aspects linked to processes or compositions used in powder metallurgy · CPC title
Fe-Si based alloys · CPC title
Related publications grouped by family.