Lithium niobate and method for producing the same
US-2022123315-A1 · Apr 21, 2022 · US
US11563210B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11563210-B2 |
| Application number | US-202016992274-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 13, 2020 |
| Priority date | Aug 13, 2020 |
| Publication date | Jan 24, 2023 |
| Grant date | Jan 24, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed herein are a sulfide-based all-solid-state battery and a method of manufacturing the same, wherein the sulfide-based all-solid-state battery includes a positive electrode active material coated with a lithium niobate precursor, which is manufactured by a polyol process having low production cost, such that it improves safety and increases capacity of the sulfide-based all-solid-state battery.
Opening claim text (preview).
The invention claimed is: 1. A method of coating a positive electrode active material, comprising: S 1 ) mixing a polyol and a chelating agent with each other to form a polyol precursor; S 2 ) mixing the polyol precursor with lithium hydroxide and ammonium niobate oxalate hydrate to form a positive electrode active material coating material in a dry state; S 3 ) mixing the positive electrode active material coating material and a positive electrode active material with each other at a temperature to form a mixture, increasing the temperature to a target temperature of 450° C. to 500° C., heat-treating the mixture at the target temperature for 2 to 3 hours to obtain a coated positive electrode active material, and S 4 ) cooling the coated positive electrode active material to room temperature, wherein the polyol is a polyether polyol or a polyester polyol, and the chelating agent is citric acid, polyvinylpyrrolidone (PVP), carboxylic acid, or a weak acid including a nitrogen element. 2. The method of coating a positive electrode active material according to claim 1 , wherein in step S 3 ), the temperature is increased at a rate of 5° C. per minute to the target temperature, and in step S 4 ), the cooling of the coated positive electrode active material to the room temperature is performed through natural cooling.
as layered products · CPC title
Positive electrodes · CPC title
inorganic · CPC title