Electrode material for aluminum electrolytic capacitors and method for producing same
US-2024301561-A1 · Sep 12, 2024 · US
US11534829B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11534829-B2 |
| Application number | US-201716603520-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 7, 2017 |
| Priority date | Apr 7, 2017 |
| Publication date | Dec 27, 2022 |
| Grant date | Dec 27, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A sintered friction material is formed by pressure sintering mixed powder at 800° C. or above, the mixed powder consisting of, in mass %, Cu and/or Cu alloy: 40.0 to 80.0%, Ni: 0% or more and less than 5.0%, Sn: 0 to 10.0%, Zn: 0 to 10.0%, VC: 0.5 to 5.0%, Fe and/or Fe alloy: 2.0 to 40.0%, lubricant: 5.0 to 30.0%, metal oxide and/or metal nitride: 1.5 to 30.0%, and the balance being impurity.
Opening claim text (preview).
The invention claimed is: 1. A sintered friction material formed by pressure sintering mixed powder at 800° C. or above, the mixed powder consisting of, in mass %: Cu and/or Cu alloy: 40.0 to 80.0%; Ni: 0% or more and less than 5.0%; Sn: 0 to 10.0%; Zn: 0 to 10.0%; VC: 0.5 to 5.0%; Fe alloy and optionally Fe: 2.0 to 40.0%; lubricant: 5.0 to 30.0%; metal oxide and/or metal nitride: 1.5 to 30.0%; and the balance being impurity, wherein the Fe alloy includes stainless steel, wherein the metal oxide and/or metal nitride includes one or more kinds selected from zircon sand, silica, mullite, and silicon nitride. 2. The sintered friction material according to claim 1 , wherein the lubricant contains one or more kinds selected from graphite: 5.0 to 15.0%, hexagonal boron nitride: 3.0% or less, molybdenum disulfide: 3.0% or less, mica: 3.0% or less, and one or more kinds selected from tungsten disulfide, iron sulfide, chromium sulfide, copper sulfide, and copper matte: 10.0% or less. 3. The sintered friction material according to claim 1 , wherein the Fe alloy includes one or more kinds selected from ferrochromium, ferrotungsten, and ferromolybdenum. 4. The sintered friction material according to claim 2 , wherein the Fe alloy includes one or more kinds selected from ferrochromium, ferrotungsten, and ferromolybdenum.
characterised by the composition · CPC title
Iron · CPC title
Low melting point metals, i.e. Zn, Pb, Sn, Cd, In, Ga · CPC title