Cellulose fiber-containing resin composition, sheet, and molded body
US-2020399443-A1 · Dec 24, 2020 · US
US11447612B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11447612-B2 |
| Application number | US-201716315723-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 7, 2017 |
| Priority date | Jul 8, 2016 |
| Publication date | Sep 20, 2022 |
| Grant date | Sep 20, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The purpose of the present invention is to provide a composite sheet in which the dimension stability when it is tensed is high and the appearance deterioration and the yellowness change are suppressed. The present invention relates to a sheet comprising; cellulose fibers having a fiber width of 1000 nm or less and having a phosphoric acid group or a phosphoric acid group-derived substituent; and a polyvinyl alcohol-based resin, wherein the sheet has a tensile elastic modulus of 3.4 GPa or more.
Opening claim text (preview).
The invention claimed is: 1. A sheet comprising: cellulose fibers having a fiber width of 2 to 50 nm and having a phosphoric acid group or a phosphoric acid group-derived substituent; and a polyvinyl alcohol-based resin, wherein the sheet has a tensile elastic modulus of 4.0 GPa or more, the average degree of polymerization of the polyvinyl alcohol-based resin is 300 to 2200, the saponification degree of the polyvinyl alcohol is 50 mol % or more, the content of the cellulose fibers is 10% by mass or more with respect to the total mass of the sheet, and the sheet is made from a suspension which contains the cellulose fibers and the polyvinyl alcohol-based resin. 2. The sheet according to claim 1 , wherein the content of the polyvinyl alcohol-based resin is 9% by mass or more, with respect to the total mass of the sheet. 3. The sheet according to claim 1 , wherein the polyvinyl alcohol-based resin is a modified polyvinyl alcohol-based resin. 4. The sheet according to claim 1 , which further comprises at least any one selected from crosslinkers and crosslinker-derived functional groups. 5. The sheet according to claim 1 , wherein, when the yellowness of a sheet measured in accordance with JIS K 7373 is set at YI 1 and the yellowness of a sheet after being subjected to vacuum drying at 200° C. for 4 hours is YI 2 , the value of YI 2 −YI 1 is 70 or less. 6. The sheet according to claim 4 , wherein the content of the polyvinyl alcohol-based resin is 90% by mass or less, with respect to the total mass of the sheet.
Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids · CPC title
Manufacture of films or sheets · CPC title
with vegetable or animal fibrous material · CPC title
Cellulose; Modified cellulose · CPC title
Esters of inorganic acids · CPC title