Hard transparent thermoplastic polyurethane
US-2019359823-A1 · Nov 28, 2019 · US
US11447596B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11447596-B2 |
| Application number | US-201716462977-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 22, 2017 |
| Priority date | Dec 23, 2016 |
| Publication date | Sep 20, 2022 |
| Grant date | Sep 20, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to a thermoplastic polyurethane obtainable or obtained by reacting a polyisocyanate composition, a chain extender, and a polyol composition, wherein the polyol composition comprises a polyol (P1) which has a molecular weight Mw in the range from 1500 to 2500 g/mol and has at least one aromatic polyester block (B1). The present invention further relates to a process for producing a shaped body comprising such a thermoplastic polyurethane, and to shaped bodies obtainable or obtained by a process of the invention.
Opening claim text (preview).
The invention claimed is: 1. A thermoplastic polyurethane obtained by reacting at least the following components (i) to (iii): (i) at least one polyisocyanate composition, (ii) at least one chain extender, and (iii) at least one polyol composition, wherein the at least one polyol composition comprises a polyol (P1) which has at least one aromatic polyester block (B1) and at least one aliphatic polyester block, wherein polyol (P1) is prepared by reacting an aromatic polyester which has a higher molecular weight than the blocks (B1) present in the polyol (P1); and wherein the at least one polyol composition comprises a further polyol selected from the group consisting of a polyetherol, a polyesterol, a polycarbonate alcohol and a hybrid polyol. 2. The thermoplastic polyurethane of claim 1 , wherein the polyol (P1) comprises 10% to 50% by weight of the at least one aromatic polyester block (B1), based on a total weight of the polyol (P1). 3. The thermoplastic polyurethane of claim 1 , wherein the at least one aromatic polyester block (B1) comprises a polyester of an aromatic dicarboxylic acid and an aliphatic diol. 4. The thermoplastic polyurethane of claim 1 , wherein the at least one aromatic polyester block (B1) comprises a polyethylene terephthalate block or a polybutylene terephthalate block. 5. The thermoplastic polyurethane of claim 1 , wherein the at least one aromatic polyester block (B1) comprises a polyethylene terephthalate block. 6. The thermoplastic polyurethane of claim 1 , wherein the at least one chain extender comprises a diol having a molecular weight <220 g/mol. 7. The thermoplastic polyurethane of claim 1 , wherein the at least one chain extender and the polyol (P1) present in the at least one polyol composition are used in a molar ratio of from 40:1 to 1:10. 8. The thermoplastic polyurethane of claim 1 , wherein the at least one polyisocyanate composition comprises an aliphatic or aromatic diisocyanate. 9. A process for producing a shaped body (SC), the process comprising: (a) preparing a thermoplastic polyurethane, the preparing comprising the reaction of (i) at least one polyisocyanate composition, (ii) at least one chain extender, and (iii) at least one polyol composition, wherein the at least one polyol composition comprises a polyol (P1) which has at least one aromatic polyester block (B1) ad at least one aliphatic polyester block, wherein polyol (P1) is prepared by reacting an aromatic polyester which has a higher molecular weight than the blocks (B1) present in the polyol (P1); and wherein the at least one polyol composition comprises a further polyol selected from the group consisting of a polyetherol, a polyesterol, a polycarbonate alcohol and a hybrid polyol and (b) producing a shaped body (SC) from the thermoplastic polyurethane. 10. The process of claim 9 , wherein the shaped body (SC) of (b) is produced by extrusion, injection molding or sintering methods or from solution. 11. A shaped body obtained by the process of claim 9 . 12. The shaped body of claim 11 , wherein the shaped body is a foil or an injection molding.
characterised by the choice of material · CPC title
from mixtures or combinations of aromatic dicarboxylic acids and aliphatic dicarboxylic acids and dialcohols · CPC title
containing only one alkylene bisphenyl group · CPC title
acyclic · CPC title
containing two or more cycloaliphatic rings · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.