Foam molding resin and method for manufacturing foam molded article
US-2018215885-A1 · Aug 2, 2018 · US
US11434342B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11434342-B2 |
| Application number | US-201816640076-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 23, 2018 |
| Priority date | Aug 30, 2017 |
| Publication date | Sep 6, 2022 |
| Grant date | Sep 6, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
According to the present invention, provided is a foam molding resin containing low-density polyethylene, wherein a strain hardening degree of the low-density polyethylene is equal to or more than 0.40.
Opening claim text (preview).
The invention claimed is: 1. A method for producing a foam molded article by blow molding or vacuum molding, comprising steps of: extruding, from a foam extruder, a melt-kneaded resin obtained by melt-kneading a foam molding resin and a foaming agent in the foam extruder to form a foamed parison; and molding the foamed parison by blow molding or vacuum molding to obtain the foam molded article, wherein the foam molding resin contains low-density polyethylene, a strain hardening degree of the low-density polyethylene is equal to or more than 0.40, and melt tension of the low-density polyethylene is equal to or more than 250 mN. 2. The method of claim 1 , wherein the foam molding resin further contains high-density polyethylene. 3. The method of claim 2 , wherein a mass ratio of the low-density polyethylene and the high-density polyethylene is 2:8 to 8:2. 4. The method of claim 1 , wherein shear viscosity of the low-density polyethylene is equal to or more than 450 Pa·s. 5. A method for producing a foam molded article by blow molding or vacuum molding, comprising steps of: extruding, from a foam extruder, a melt-kneaded resin obtained by melt-kneading a foam molding resin and a foaming agent in the foam extruder to form a foamed parison; and molding the foamed parison by blow molding or vacuum molding to obtain the foam molded article, wherein the foam molding resin contains low-density polyethylene, a strain hardening degree of the low-density polyethylene is equal to or more than 0.40, and shear viscosity of the low-density polyethylene is equal to or more than 450 Pa·s. 6. The method of claim 5 , wherein the foam molding resin further contains high-density polyethylene. 7. The method of claim 6 , wherein a mass ratio of the low-density polyethylene and the high-density polyethylene is 2:8 to 8:2. 8. The method of claim 5 , wherein melt tension of the low-density polyethylene is equal to or more than 250 mN.
characterised by the die · CPC title
characterised by the material · CPC title
Extrusion blow-moulding · CPC title
containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure · CPC title